Porosity of resin veneer materials

&
Pages 321-328 | Received 13 Oct 1986, Published online: 02 Jul 2009
 

Abstract

The present investigation has studied the effects of different types of resins and different processing and curing methods on the number and size of pores occurring in resin facing materials. The mean number of pores per square millimeter varied between 0.5 and 4. The highest numbers occurred in unfilled heat-polymerized acrylic resin and in light-activated resin, whereas the lowest numbers were found in heat-polymerized micro-filled resin. Specimens processed in accordance with the free technique and cured under pressure consistently obtained lower numbers of pores than the corresponding specimens processed in a flask. Most of the pores were less than 50 μm in diameter in all test groups. From a clinical point of view, a dense resin with a limited content of pores may give the most favorable results in terms of mechanical, esthetic, and hygienic properties of the veneer. □ Crowns; dental materials; dental resins; fixed prosthodontics; processing methods

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.