Fracture strength of porcelain fused to metal crowns made of cast, milled or laser-sintered cobalt-chromium

&
Pages 1280-1289 | Received 29 Aug 2012, Accepted 08 Nov 2012, Published online: 16 Jan 2013

References

  • Haselton DR, Diaz-Arnold AM, Dunne JT Jr. Shear bond strengths of 2 intraoral porcelain repair systems to porcelain or metal substrates. J Prosthet Dent 2001;86:526–31.
  • Bagby M, Marshall SJ, Marshall GW Jr. Metal ceramic compatibility: a review of the literature. J Prosthet Dent 1990;63:21–5.
  • dos Santos JG, Fonseca RG, Adabo GL, dos Santos Cruz CA. Shear bond strength of metal-ceramic repair systems. J Prosthet Dent 2006;96:165–73.
  • Chung KH, Hwang YC. Bonding strengths of porcelain repair systems with various surface treatments. J Prosthet Dent 1997;78:267–74.
  • Lombardo GH, Nishioka RS, Souza RO, Michida SM, Kojima AN, Mesquita AM, et al. Influence of surface treatment on the shear bond strength of ceramics fused to cobalt-chromium. J Prosthodont 2010;19:103–11.
  • Joias RM, Tango RN, Junho de Araujo JE, Junho de Araujo MA, Ferreira Anzaloni Saavedra Gde S, Paes-Junior TJ, et al. Shear bond strength of a ceramic to Co-Cr alloys. J Prosthet Dent 2008;99:54–9.
  • Quante K, Ludwig K, Kern M. Marginal and internal fit of metal-ceramic crowns fabricated with a new laser melting technology. Dent Mater 2008;24:1311–15.
  • de Melo RM, Travassos AC, Neisser MP. Shear bond strengths of a ceramic system to alternative metal alloys. J Prosthet Dent 2005;93:64–9.
  • Salazar MSM, Pereira SM, Ccahuana VVZ, Passos SP, Vanderlei AD, Pavanelli CA, et al. Shear bond strength between metal alloy and a ceramic system, submitted to different thermocycling immersion times. Acta Odontol Latinoam 2007;20:97–102.
  • Ozcan M. Fracture reasons in ceramic-fused-to-metal restorations. J Oral Rehabil 2003;30:265–9.
  • Tan K, Pjetursson BE, Lang NP, Chan ES. A systematic review of the survival and complication rates of fixed partial dentures (FPDs) after an observation period of at least 5 years. Clin Oral Implants Res 2004;15:654–66.
  • Kelly JR. Dental ceramics: current thinking and trends. Dent Clin North Am 2004;48:513–30.
  • Geminiani A, Lee H, Feng C, Ercoli C. The influence of incisal veneering porcelain thickness of two metal ceramic crown systems on failure resistance after cyclic loading. J Prosthet Dent 2010;103:275–82.
  • Roberts HW, Berzins DW, Moore BK, Charlton DG. Metal-ceramic alloys in dentistry: a review. J Prosthodont 2009;18:188–94.
  • Walton TR. An up to 15-year longitudinal study of 515 metal-ceramic FPDs: Part 1. Outcome. Int J Prosthodont 2002;15:439–45.
  • de Vasconcellos LG, Buso L, Lombardo GH, Souza RO, Nogueira L Jr, Bottino MA, et al. Opaque layer firing temperature and aging effect on the flexural strength of ceramic fused to cobalt-chromium alloy. J Prosthodont 2010;19:471–7.
  • Wu Y, Moser JB, Jameson LM, Malone WF. The effect of oxidation heat treatment of porcelain bond strength in selected base metal alloys. J Prosthet Dent 1991;66:439–44.
  • Pretti M, Hilgert E, Bottino MA, Avelar RP. Evaluation of the shear bond strength of the union between two CoCr-alloys and a dental ceramic. J Appl Oral Sci 2004;12:280–4.
  • do Prado RA, Panzeri H, Fernandes Neto AJ, das Neves FD, da Silva MR, Mendonca G. Shear bond strength of dental porcelains to nickel-chromium alloys. Braz Dent J 2005;16:202–6.
  • Ucar Y, Akova T, Akyil MS, Brantley WA. Internal fit evaluation of crowns prepared using a new dental crown fabrication technique: laser-sintered Co-Cr crowns. J Prosthet Dent 2009;102:253–9.
  • Wataha JC. Alloys for prosthodontic restorations. J Prosthet Dent 2002;87:351–63.
  • van Noort R. Introduction to Dental Materials. 3rd edn. Edinburgh: Mosby; 2007.
  • Akova T, Ucar Y, Tukay A, Balkaya MC, Brantley WA. Comparison of the bond strength of laser-sintered and cast base metal dental alloys to porcelain. Dent Mater 2008;24:1400–4.
  • Viennot S, Dalard F, Lissac M, Grosgogeat B. Corrosion resistance of cobalt-chromium and palladium-silver alloys used in fixed prosthetic restorations. Eur J Oral Sci 2005;113:90–5.
  • Ortorp A, Jonsson D, Mouhsen A, Vult von Steyern P. The fit of cobalt-chromium three-unit fixed dental prostheses fabricated with four different techniques: a comparative in-vitro study. Dent Mater 2010;27:356–63.
  • Willer J, Rossbach A, Weber HP. Computer-assisted milling of dental restorations using a new CAD/CAM data acquisition system. J Prosthet Dent 1998;80:346–53.
  • Miyazaki T, Hotta Y, Kunii J, Kuriyama S, Tamaki Y. A review of dental CAD/CAM: current status and future perspectives from 20 years of experience. Dent Mater J 2009;28:44–56.
  • Samet N, Resheff B, Gelbard S, Stern N. A CAD/CAM system for the production of metal copings for porcelain-fused-to-metal restorations. J Prosthet Dent 1995;73:457–63.
  • Rosentritt M, Behr M, Thaller C, Rudolph H, Feilzer A. Fracture performance of computer-aided manufactured zirconia and alloy crowns. Quintessence Int 2009;40:655–62.
  • Strub JR, Rekow ED, Witkowski S. Computer-aided design and fabrication of dental restorations: current systems and future possibilities. J Am Dent Assoc 2006;137:1289–96.
  • Kellerhoff RK, Fischer J. In-vitro fracture strength and thermal shock resistance of metal-ceramic crowns with cast and machined AuTi frameworks. J Prosthet Dent 2007;97:209–15.
  • Xie H, Yuan X, Wu F. Effects of surface treatments on bond strength between porcelain and electroformed gold substrates. J Adhes Dent 2009;11:485–91.
  • Fischer J, Zbaren C, Stawarczyk B, Hammerle CH. The effect of thermal cycling on metal-ceramic bond strength. J Dent 2009;37:549–53.
  • Fernandes Neto AJ, Panzeri H, Neves FD, Prado RA, Mendonca G. Bond strength of three dental porcelains to Ni-Cr and Co-Cr-Ti alloys. Braz Dent J 2006;17:24–8.
  • Wagner WC, Asgar K, Bigelow WC, Flinn RA. Effect of interfacial variables on metal-porcelain bonding. J Biomed Mater Res 1993;27:531–7.
  • Schweitzer DM, Goldstein GR, Ricci JL, Silva NR, Hittelman EL. Comparison of bond strength of a pressed ceramic fused to metal versus feldspathic porcelain fused to metal. J Prosthodont 2005;14:239–47.
  • Huang HH, Lin MC, Lee TH, Yang HW, Chen FL, Wu SC, et al. Effect of chemical composition of Ni-Cr dental casting alloys on the bonding characterization between porcelain and metal. J Oral Rehabil 2005;32:206–12.
  • Vult von Steyern P, Ebbesson S, Holmgren J, Haag P, Nilner K. Fracture strength of two oxide ceramic crown systems after cyclic pre-loading and thermocycling. J Oral Rehabil 2006;33:682–9.
  • Oliveira de Vasconcellos LG, Silva LH, Reis de Vasconcellos LM, Balducci I, Takahashi FE, Bottino MA. Effect of airborne-particle abrasion and mechanic-thermal cycling on the flexural strength of glass ceramic fused to gold or cobalt-chromium alloy. J Prosthodont 2011;20:553–60.
  • Johnson T, van Noort R, Stokes CW. Surface analysis of porcelain fused to metal systems. Dent Mater 2006;22:330–7.
  • Mehulić K, Lauš–Šošić M, Schauperl Z, Vojvodić D, Štefančić S. Influence of cast surface finishing process on metal-ceramic bond strength. Med Glas 2009;6:235–42.
  • Larsson C. Zirconium Dioxide Based Dental Restorations: Studies on Clinical Performance and Fracture Behavior [Dissertation]. Malmö: Malmö University; 2011.
  • Webber B, McDonald A, Knowles J. An in-vitro study of the compressive load at fracture of Procera AllCeram crowns with varying thickness of veneer porcelain. J Prosthet Dent 2003;89:154–60.
  • Sobrinho LC, Cattell MJ, Knowles JC. Fracture strength of all-ceramic crowns. J Mater Sci Mater Med 1998;9:555–9.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.