Abstract
The paper reports the results of the temperature dependence measurements of the specific heat for a SrTiO3 thin (104 nm) film deposited on a DyScO3 substrate. Two anomalies of the specific heat have been observed. They can be associated with the strain-induced ferroelectric phase transition (at 304K) and the shifted antiferrodistortive structural phase transition (at 173 K).
Acknowledgments
The authors would like to express their sincere gratitude to Professor Mario Maglione for his promotional suggestion to run this work. Authors express their gratitude to Russian Foundation for Basic Research for financial support (project no. 08-02-01010) and the Dutch Foundation for Fundamental Research on Matter (FOM) and the Netherlands Organization for Scientific Research (NOW-Vidi Grant).