Ferroelectric Fatigue of KNN Ceramics

, , , , , , & show all
Pages 119-125 | Accepted 03 Dec 2014, Published online: 01 Sep 2015
 

Abstract

Phase-pure KNN (K0.5Na0.5NbO3) was synthesized from Rochelle salt and niobium pentoxide through solid-state route and the synthesized powder was sintered at 1130°C to get dense KNN ceramics. After polarization fatigue test, it was found that the d33, kP and remanent polarization (Prem) of KNN decreased substantially. The reduction of the aforesaid parameters after fatigue was much higher in comparison to that of soft PZT (Navy type VI) tested under identical conditions. The possible reason behind such behaviour has been delineated.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.