Studies on Seebeck Effect in erbium doped silver vanadate

, &
Pages 175-178 | Received 05 Oct 1995, Published online: 07 Mar 2011
 

Abstract

The Seebeck Effect has been observed in ferroelectric ceramic of silver vanadate doped with various concentrations of erbium oxide, in the temperature range covering the phase transition temperature, by maintaining the thermal gradient across the sample by using a subheater. It has been investigated that with the change of temperature of the samples the Seebeck coefficient changes, it becomes positive in ferroelectric region and negative in paraelectric region of the samples. Also it has been observed that the Seebeck coefficients are having different peak values for samples containing different concentrations of erbium oxide in silver vanadate. The Seebeck coefficient decreases to zero, indicating the phase transition temperature of the sample. Pure as well as erbium doped silver vanadate samples show p-type behaviour in ferroelectric region and n-type behaviour in the paraelectric region.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.