Effects of structural parameters on compressibility and soiling properties of machine woven carpets

ORCID Icon, , &
Pages 1263-1270 | Received 13 Aug 2018, Accepted 03 Dec 2018, Published online: 29 Jan 2019
 

Abstract

Compressibility performance of the machine woven carpet after a static or dynamic loading expresses the texture deformation tendency of the carpet. This study is an experimental attempt to investigate the effects of pile height and pile density on compressibility and soiling property by dynamic loading, prolonged heavy static loading, compression recovery and artificial soiling tests. In this study, a total of 12 carpet samples with three different pile heights and four different pile densities were tested. As a result of this study, it was seen that higher pile density provides a lower thickness loss and so a lower level of texture deformation. On the other hand, pile height has a preventing effect for texture deformation for static loading and compression recovery tests whereas there is no considerable effect on dynamic loading test. There is no considerable difference between the soiling properties of the samples.

Disclosure statement

No potential conflict of interest was reported by the authors.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.