Influence factors of X80 pipeline steel girth welding with self-shielded flux-cored wire

, , , , &
Pages 592-601 | Received 10 May 2016, Accepted 13 Sep 2016, Published online: 31 Oct 2016
 

Abstract

For girth weld of high-pressure oil and gas transmission pipeline, there is impact toughness values deviation phenomenon with self-shielded flux-cored semi-automatic welding technology. The macro-images, microstructure and mechanical performance of girth welding joint have been investigated by OM, SEM, TEM. The results show that there are several factors of impact toughness unqualified values of weld joints, such as welding heat input, coarse grain zone and a chain of M–A organisations, Al2O3 and Zr Precipitates particle sizes and distribution et al., which are the main unqualified reasons of welding impact toughness of the semi-automatic self-shielded core butt welding process of X80 pipeline steel.

Acknowledgement

This work was supported by the Science research and technology development project of CNPC (No. 2014B-3416-0501) and Project of Natural Science Foundation of Shaanxi Province in China (2012GY2-23).

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.