A multiscale-indentation study of deformation and fracture in 6H polycrystalline silicon carbide

, ORCID Icon &
Pages 1111-1124 | Received 10 Dec 2019, Accepted 08 Apr 2020, Published online: 24 Apr 2020
 

ABSTRACT

The mechanical behaviour of a polycrystalline silicon carbide across length scales was studied using Vickers indentation, focusing on the hardness, fracture toughness and failure mechanism of the material. For macroscopic and microscopic indentations, the hardness decreased with an increase in load, which was associated with the well-known indentation size effect as well as the internal flaws. For nanoindentation, severe plastic deformation was discovered beneath the imprints on the basal plane (0001) which is the most favourable crystallographic plane for dislocation movement. Alternative sources of plastic deformation, including deformation twinning and stacking faults, were found for nanoindentations with an increased load. Also, cracking was observed for indents made at 100 mN and above, which was used to study the fracture toughness.

Acknowledgement

The authors acknowledge the use of facilities within the Loughborough Materials Characterisation Centre.

Disclosure statement

No potential conflict of interest was reported by the authors.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.