Enhancement of pearlite transformation by Warm Rolling in 1.0C-1.5Cr Steel

, , , &
Pages 1431-1439 | Received 08 Nov 2019, Accepted 27 Jun 2020, Published online: 09 Jul 2020
 

Abstract

Isothermal and non-isothermal pearlite transformations under 840°C warm-rolled and 950°C hot-rolled were researched. It was found that the pearlite nuclei at grain boundary and defects were increased by warm deformation. The results showed that the incubation time was shortened in the isothermal pearlite transformation and the volume fraction of pearlite was increased in continuous cooling condition by warm deformation. The pearlite transformation behaviour under continuous cooling condition was predicted by the formula of Umemoto. The critical cooling rates of the fully pearlite structures formed under warm deformation condition and hot deformation condition were calculated.

Acknowledgements

This work was supported by the National Key R&D Program of China [grant number 2017YFB0304201].

Disclosure statement

No potential conflict of interest was reported by the author(s).

Additional information

Funding

This work was supported by the National Key R&D Program of China [grant number 2017YFB0304201].

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.