Synthesis and Dielectric Properties of a Temperature Stable Ceramic: Ba4La3.73Sm4.66Bi0.93Ti18O54

&
Pages 31-37 | Received 14 Jan 2012, Accepted 30 May 2012, Published online: 11 Sep 2012
 

Abstract

A temperature stable high dielectric constant Ba4La3.73Sm4.66Bi0.93Ti18O54 ceramic was synthesized by conventional solid state route. The structural and micro-structural properties were investigated by X-ray diffraction (XRD) and scanning electron microscopy (SEM). The compound crystallizes in the orthorhombic system with unit cell parameters as a = 12.56Å, b = 22.25Å, c = 3.83Å and v = 1070.33Å3. The microwave dielectric properties were measured in the frequency range 0.3 to 3.0 GHz using a network analyzer and it shows a high dielectric constant of 86.1 and low loss tangent of 4.3 × 10–3 at 3.0 GHz along with a very low temperature coefficient of resonant frequency of 4.3 ppm/°C. It could be a promising candidate to be used as dielectric resonator in microwave communication.

Acknowledgments

Communicated by Dr. Deborah J. Taylor

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.