Abstract
Methods of friction welding creep-resisting deformable nickel alloys and heat treatment are investigated. Welding conditions are selected. The results of mechanical tests and the determination of short- and long-term strength and impact bending resistance are presented, and the data obtained in metallographic and fractographic studies of the welded joints are described.