Abstract

The formation of stable back beads in a root pass weld during one side multi-layer welding is important to achieve high quality welded metal joints in MAG welding. The authors employed the switch back welding method for V groove joints without backing plates. In this switch back welding method, the torch moves forward and backward with an oscillation frequency of 2.5 Hz. In order to achieve this welding, personal computers control the conventional welding robot, the power source characteristic and the wire feeder unit. During the forward, the torch is weaving on the V groove gap without the weld pool. If the weaving width becomes wider than the proper width, the tip of the wire becomes high and a good back bead cannot be obtained. The weaving width is adjusted so as to get the proper width in the switch back welding. The suitability of the welding conditions for each root gap was verified by observation of the arc, the weld pool and the external appearance of back beads. A good back bead was obtained under V groove welding in 2–4 mm gap.

Notes

Presented at the Autumn National Conference 2009; Presented at the Welding Research Committee, February 2010.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.