Solvent deasphalting of Saudi residue to produce 30# hard asphalt

, , &
 

ABSTRACT

30# asphalts produced directly by de-oiled asphalt (DOA) showed poor ductility at low temperature and deasphalted oil (DAO) yield was below 17.6%. Combination technology of solvent deasphalting and blending was investigated to produce 30# asphalt and results demonstrated that the 30# blended asphalt with Saudi residue and DOA prepared under conditions of temperature of 105°C, pressure of 4.0 MPa, and solvent/VR ratio of 5 conformed to GB/T 15180–2010 and its asphalt mixture had excellent rutting resistance and water stability performance; meanwhile, DAO yield reached 42.7% and good quality DAO satisfied the feedstock requirement for catalytic cracking process.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.