Dimensional stabilization of compressed laminated veneer lumber by hot pressing in an airtight frame

, , &
Pages 119-125 | Received 22 Oct 2007, Published online: 16 Jun 2009
 

Abstract

The purpose of this study was to evaluate the dimensional stability and strength properties of compressed laminated veneer lumber (LVL) produced using a closed hot pressing system. LVL specimens were produced with varying number of veneers using either diphenylmethane diisocyanate (MDI) or a water-soluble phenol formaldehyde (PF) resin at varying temperatures (160–200°C), pressures (0.5–3 MPa) and hot-pressing times (2–16 min). Results show that the heating process decreases the recovery of compressive deformation in the veneers when subjected to cyclic moisture and heat conditions. Thickness swelling was approximately 5% after a drying, wetting and boiling cyclic test for LVL using the MDI resin and hot pressed at 200°C for 8 min. Modulus of elasticity and rupture increased for samples produced in both an open press and the closed press with an increase in the number of veneers and density, as did the absorbed energy in impact bending.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.