Influence of sintering conditions on tensile and high cycle fatigue behaviour of powder injection moulded Ti–6Al–4V at ambient and elevated temperatures

, &
Pages 283-290 | Received 15 Apr 2014, Accepted 15 Jun 2014, Published online: 11 Jul 2014
 

Abstract

Tensile and high cycle fatigue properties of Ti–6Al–4V samples fabricated by powder injection moulding (PIM) are examined at room temperature and elevated temperatures. Standard wrought Ti–6Al–4V material is used for comparison. The tensile and the fatigue strength of samples fabricated by powder injection moulding are found to be significantly lower than conventional wrought material. On the other hand, strength and ductility of metal injection moulded (MIM) samples are high enough to be of large practical interest, in particular if the low processing costs for intricate shapes are taken into account. The inferior properties of the MIM material are caused by considerable remaining porosity, enlarged grain size and increased interstitial content. Prolonged sintering times lead to improved density and strength. At the same time, the room temperature ductility is observed to drop to very low levels, presumably because of additional grain growth.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.