Impact of ribbon width on magnetoimpedance and permeability of Fe69.2Co7.7Cu0.6Nb2.5Si11B9 soft magnetic alloy

, , , , &
Pages 337-341 | Received 27 Mar 2015, Accepted 02 Jul 2015, Published online: 02 Feb 2016
 

Abstract

Fe69.2Co7.7Cu0.6Nb2.5Si11B9 soft magnetic alloy ribbons of different widths, 4.4 and 8.0 mm respectively, were used for the research work. The influences of structural modifications induced by heat treatment on magnetoimpedance effect and permeability have been studied. In as quenched state and annealed at temperatures < 773 K, 4.4 mm wide ribbons showed larger MI values than the 8.0 mm wide ribbons. After being annealed at temperatures >823 K, the MI values of the 8.0 mm wide ribbons were slightly higher than those of 4.4 mm wide ribbons due to the improved soft magnetic properties. With controlled heat treatment at 853 K, a maximum MI ratio of 82% was detected for the 8.0 mm wide ribbon.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.