Silicon carbide whisker reinforced aluminium composites–fabrication and properties

Pages 57-60 | Published online: 02 Dec 2013
 

Abstract

A fabrication process for SiC whisker reinforced aluminium composites is being developed. Theftrst step involves preforming the SiC whisker and squeeze-infiltrating the molten metal into the preform. Secondary fabrication can involve a conventional hot metal working practice such as extrusion. Microscopic observations indicate that the distribution of whiskers is very homogeneous. In an aluminium alloy (AA 6061) matrix composite containing 17 vol.-% SiC whiskers, the Young's modulus is > 100 GPa and the tensile strength increases by ~ 50–70% above that of the matrix to 460 and 529 MN m−2 in the cast and extruded products, respectively. The strength at elevated temperature and the wear resistance are also improved. These enhanced properties make the composite potentially suitable for a number of automotive applications.

MST/574

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.