Spent nuclear fuel transport and/or storage containers (casks) must maintain their structural integrity even when subjected to hypothetical accidents during transport or handling accidents at storage facilities. For ductile cast iron (DCI) to be used as a cask containment boundary material, adequate fracture toughness must be demonstrated at service temperatures and Impact loading conditions of concern. In Japan, comprehensive studies of the fracture toughness of heavy section DCI have been undertaken by a number of research organisations to provide the safety assurance for the DCI casks. In the present study, the fracture toughness data were used to develop a lower bound trend curve for heavy section DCI and to examine the prediction methods by small specimen tests. The fracture toughnesses KIc, KIIc and KIIIc were also obtained to study the safety assessment of DCI casks under different loading mode conditions.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.