C.2. Creep Property

Creep Rupture Properties of Superalloys Developed for Nuclear Steelmaking

, , , , &
Pages 260-272 | Published online: 13 May 2017
 

Abstract

Creep rupture tests on six candidate alloys for intermediate heat exchangers of high-temperature gas-cooled reactors were carried out at 1173 to 1323 K in helium with small amounts of H2, CH4, CO, and C02, and at 1173K in H2 + 15% CO + 5% C02. The creep rupture strengths of each alloy were scarcely different at 1173 K in both environments. At higher temperatures in helium environments, the degradation of the creep rupture strengths appeared in carbide-strengthened alloys because of decarburization. The alloy, which mainly uses α-W as a strengthener, showed stable creep rupture strength up to 1323 K in spite of severe decarburization.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.