A hydroxyethyl methacrylate monomer medium incorporating 2-butoxyethanol requires 2 stock solutions for embedding. Solution A: 80 ml of hydroxyethyl methacrylate (Rohm and Haas Co., Philadelphia, Pa.) is mixed well with 16 ml of 2-butoxyethanol; 0.27 gm of benzoyl peroxide, the catalyst, is added and permitted to dissolve. Heating to 40–50 C may be used to accelerate its solution. Solution B: polyethylene glycol 200 or 400, 15 parts, and N,N-dimethylaniline, 1 part, are mixed thoroughly. Tissues are dehydrated in the customary manner to absolute ethanol or other comparable dehydrant, infiltrated completely with A, then cast in a mixture consisting of 42 parts of A well mixed with 1 part of B. Polymerizaion occurs in 4–7 hr. In a water bath at 20 C the time required was about 7 hr; at 28 C, 4 hr. This medium is based on the author's water-polyethylene glycol-hydroxyethyl methacrylate monomer medium (Stain Techn., 42: 119–23, 1967).

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.