Effect of the aspect ratio of the pre-existing rectangular adhesion failure on the structural integrity of the adhesively bonded single lap joint

ORCID Icon, &
Pages 2093-2111 | Received 14 Mar 2019, Accepted 31 May 2019, Published online: 26 Jun 2019
 

Abstract

Non-linear three dimensional (3-D) finite element analyses (FEA) of the single lap joints (SLJs) having pre-existing rectangular adhesion failure in the interface of the strap adherend and the adhesive have been carried out. The effect of the size, the shape and the aspect ratio of the pre-existing rectangular adhesion failure on (i) the strength, (ii) the interfacial stresses and (iii) the strain energy release rates (SERRs) in the vicinity of the adhesion failure front have been presented in this research work. The SLJ is subjected to uniformly applied tensile load. The adherends are made with very high strength steels and the adhesive is a commercially available AV119. The analyses of the adhesion failure propagation have been carried out by sequentially releasing the constraints of the nodes ahead of the pre-existing adhesion failure front in finite element model. The SERR values in the vicinity of the adhesion failure fronts are computed using the virtual crack closure technique (VCCT) for assessment of the structural integrity of the SLJ. The strength of the SLJ, the interfacial stresses, and the three modes of strain energy release rates (SERRs) have been found to be significantly affected by the shape and size of adhesion failures. The SERRs and interfacial stresses along the rectangular adhesion failure front are compared with the corresponding values around the circular adhesion failure front of same area, pre-existing in the SLJ. It is observed that the circular and rectangular adhesion failures of the same area will have dissimilar growth rate and the mode II is the dominant failure mode. The total strain energy release rate and the failure strength, computed from the 3-D FEA of the SLJ is in good agreement with the experimental fracture toughness of the AV119 adhesive and the experimentally obtained failure loads, respectively.

Disclosure statement

No potential conflict of interest was reported by the authors.

Log in via your institution

Log in to Taylor & Francis Online

PDF download + Online access

  • 48 hours access to article PDF & online version
  • Article PDF can be downloaded
  • Article PDF can be printed
USD 61.00 Add to cart

Issue Purchase

  • 30 days online access to complete issue
  • Article PDFs can be downloaded
  • Article PDFs can be printed
USD 432.00 Add to cart

* Local tax will be added as applicable

Related Research

People also read lists articles that other readers of this article have read.

Recommended articles lists articles that we recommend and is powered by our AI driven recommendation engine.

Cited by lists all citing articles based on Crossref citations.
Articles with the Crossref icon will open in a new tab.