Fig. 2 Flexural strength and fracture toughness of laminated Ti/Al2O3 composite with different amount of layers.
![](/cms/asset/6a28cf21-e0e7-4b78-827c-85199d222ce6/tace_a_12001046_f0010_ob.jpg)
Fig. 4 The crack branch, crack deflection (a) and crack deflection angle (b) of laminated Ti/Al2O3 composite after the bending test.
![](/cms/asset/c7e87f37-c663-4437-91ca-0fee125eec1d/tace_a_12001046_f0020_ob.jpg)
Fig. 5 Crack bifurcation (a), crack termination (b) and interface dissociation (c) in crack propagation paths.
![](/cms/asset/984d8a0b-abed-476f-9dc2-9c41357dc6d8/tace_a_12001046_f0025_ob.jpg)