ABSTRACT
The combined effect of nano-SiO2 and nano-Al2O3 as fillers on the tribological properties of Kevlar fabric/phenolic laminate (KFPL) in water was investigated. Results showed that the single addition of nano-SiO2 at a proper content decreased the friction coefficient of KFPL to an ultralow value at the cost of an increased wear rate. The single addition of nano-Al2O3 at a proper content reduced the wear rate of KFPL with fluctuation in the friction coefficient curve. The combined addition of nano-SiO2 and nano-Al2O3 not only endowed KFPL with an ultralow friction coefficient originated from nano-SiO2 but also improved the wear resistance. This means that the combined addition of nano-SiO2 and nano-Al2O3 can have positive effects and inhibit their negative aspects to some extent.
Funding
The research was financially supported by the National Basic Research Program of China (“973” Program, Grant No. 2014CB643302).