Abstract
The original magnesium titanate powders were pre-sintered, and the 0.95MgTiO3-0.05CaTiO3 (95MCT) ceramics were prepared by the pre-sintered magnesium titanate showed better dielectric properties than by the original powders. Because the magnesium titanate (MgTi2O5) phase was not detected. Then the microwave patch antenna was designed by the prepared ceramic measured at 2.8 GHz exhibited a 4.83% bandwidth (return loss ≤ −3 dB) of the center frequency.