Abstract
The purpose of this article is to present energetic properties of surface Ti6Al4V titanium as well as surface EN-AW-2017A(PA6) aluminum alloy layers. Values of surface free energy after selected mechanical operations and ozonation were compared. In addition, the influence of different values of ozone concentration on surface layer energetic activation was analyzed. Dispersive and polar components of surface free energy were of particular concern. Comparative evaluation of shearing strength of Ti6Al4V titanium and EN-AW-2017A(PA6) aluminum alloy single-lap adhesive bonded joints were presented. Results can be used as pro-ecological methods of titanium and aluminum alloys preparing for applications where adhesive phenomenon is important.
ACKNOWLEDGMENTS
The authors thank the financial support from the Ministry of Science and Higher Education of Poland, 2965/B/T02/2010/39.