A Review on the Recovery of Titanium Dioxide from Ilmenite Ores by Direct Leaching Technologies

&
Pages 231-247 | Published online: 30 Jul 2018
 

ABSTRACT

Pretreatment of ilmenite are required to enhance leaching efficiency of ilmenite. Strong acid leaching is promising in terms of the purity of the produced TiO2, low energy consumption and waste management. The effect of several factors on the acid leaching kinetics in reported processes was reviewed. Temperature, time and acid concentration significantly affect the dissolution of titanium and impurities in ilmenite. The addition of either iron powder or chloride/sulfate salts affects significantly the leaching rate of ilmenite. Either HCl leaching followed by solvent extraction or alkaline leaching followed by hydrolysis-calcination is recommended for the production of pure TiO2 from ilmenite. 

Additional information

Funding

This work was supported by the Global Excellent Technology Innovation of the Korea Institute of Energy Technology Evaluation and Planning (KETEP), granted financial resource from the Ministry of Trade, Industry & Energy, Republic of Korea [No.20165010100880].

Log in via your institution

Log in to Taylor & Francis Online

PDF download + Online access

  • 48 hours access to article PDF & online version
  • Article PDF can be downloaded
  • Article PDF can be printed
USD 61.00 Add to cart

Issue Purchase

  • 30 days online access to complete issue
  • Article PDFs can be downloaded
  • Article PDFs can be printed
USD 1,048.00 Add to cart

* Local tax will be added as applicable

Related Research

People also read lists articles that other readers of this article have read.

Recommended articles lists articles that we recommend and is powered by our AI driven recommendation engine.

Cited by lists all citing articles based on Crossref citations.
Articles with the Crossref icon will open in a new tab.