Abstract
The problems of producing high-strength permanent joints in dissimilar nickel-based alloys are investigated. The results of investigation of the effect of the brazing and heat treatment conditions on the structure of the brazed joints in the EP975 deformed alloy and VKNA-1U intermetallic single crystal alloy are presented.