Fractographic evaluation of high cycle fatigue strength of a high V alloyed powder metallurgy tool steel

, , &
Pages 95-100 | Received 10 May 2011, Accepted 10 Sep 2011, Published online: 12 Nov 2013
 

Abstract

The high cycle fatigue strength and the fracture surface morphology of a high V alloyed powder metallurgy tool steel were investigated and connected with microstructure. The inclusion with size above 30 μm was demonstrated to be responsible for the reduction in fatigue strength. The shape and size of inclusion and the stress amplitude affected the position of crack origin in fish eye. Based on fractographic evaluation and statistical analysis, the most harmful inclusions with the largest size proportion for steel A are ∼30 μm, and that of B1, B2 and B3 is roughly 50, 60 and 60 μm respectively. A distinctive granular-like zone with specific morphology was found to be confined in a very small area, suggesting that the fatigue crack propagation was mainly controlled by Paris Law regime. A linear fracture mechanics approach was implemented to evaluate the effect of grain size, yield stress and inclusion size on fatigue strength.

This work was financially supported by the National Key Technologies Research and Development Program (grant no. 2007BAE51B05).

Log in via your institution

Log in to Taylor & Francis Online

There are no offers available at the current time.

Related Research

People also read lists articles that other readers of this article have read.

Recommended articles lists articles that we recommend and is powered by our AI driven recommendation engine.

Cited by lists all citing articles based on Crossref citations.
Articles with the Crossref icon will open in a new tab.