140
Views
5
CrossRef citations to date
0
Altmetric
Original Articles

Impact of the Structural Changes on the Fracture Behavior of Naturally Weathered Low-Density Polyethylene (LDPE) Films

, , , , , , & show all
Pages 400-424 | Received 12 Feb 2017, Accepted 29 Dec 2018, Published online: 24 Jan 2019

References

  • Sampers, J. Importance of Weathering Factors Other than UV Radiation and Temperature in Outdoor Exposure. Polym. Degrad. Stab. 2002, 6, 455–465.
  • Lemaire, J.; Arnaud, R.; Gardette, J. L. The Role of Hydroperoxides in Photooxidation of Polyolefins, polyamides and Polyurethane Elastomers. Pure Appl. Chem 1983, 55, 1603–1614.
  • Gugumus, F. Monitoring the Influence of Different Weathering Conditions on Polyethylene Pipes by IR-Microscopy. Angew. Makromol. Chemie. 1988, 158, 151–176.
  • Gugumus, F. Mechanisms of Photooxidation of Polyolefins. Angew. Makromol. Chemie 1990, 176, 27–42.
  • Gugumus, F. Photooxidation of Polyethylene Films, 1. Experimental Kinetics of Functional Group Formation. Macromol. Mater. Eng 1990, 182, 85–109.
  • Tidjani, A. Comparison of Formation of Oxidation Products during Photo-oxidation of Linear Low-density Polyethylene under Different Natural and Accelerated Weathering Conditions. Polym. Degrad. Stab 2000, 68, 465–469.
  • Chabira, S. F.; Sebaa, M.; G'sell, C. Influence of Climatic Ageing on the Mechanical Properties and the Microstructure of Low-density Polyethylene Films. J. Appl. Polym. Sci. 2008, 110, 2516–2524.
  • Fayolle, B.; Verdu, J. EWF Method to Study Long-term Fracture Properties of Cross-linked Polyethylene. Polym. Eng. Sci. 2005, 45, 424–431.
  • Karger-Kocsis, J.; Czigány, T.; Moskala, E. J. Deformation Rate Dependence of the Essential and Non-essential Work of Fracture Parameters in an Amorphous Copolyester. Polymer 1998, 39, 3939–3944.
  • Fasce, L.; Bernal, C.; Frontini, P.; Mai, Y-w. On the Impact Essential Work of Fracture of Ductile Polymers. Polym. Eng. Sci. 2001, 41, 1–14.
  • Pettarin, V.; Frontini, P. M.; Eliçabe, G. E. Optimal Ligament Lengths in Impact Fracture Toughness Estimation by the Essential Work of Fracture Method. Polym. Test 2005, 24, 189–196.
  • G’sell, C.; Hiver, J. M. Dispositif de caractérisation optique du comportement mécanique local d’une structure pouvant présenter des déformations finies nonhomogènes, Brevet numéro 010542100 déposé à l’INPI, 2001.
  • G'Sell, C.; Hiver, J. M.; Dahoun, A. Experimental Characterization of Deformation Damage in Solid Polymers under Tension, and Its Interrelation with Necking. Int. J. Sol. Struct 2002, 39, 3857–3872.
  • Verdu, J. Vieillissement Des Plastiques; Afnor Technique, 1984., Ed., Eyrolles: Paris.
  • Fayolle, B.; Colin, X.; Audouin, L.; Verdu, J. Mechanism of Degradation Induced Embrittlement in Polyethylene. Polym. Degrad. Stab 2007, 92, 231–238.
  • Qureshi, F. S.; Amin, M. B.; Maadhah, A. G.; Hamid, S. H. Weather-induced Degradation of Linear Low-density Polyethylene: mechanical Properties. Polym. Plast. Tech. Eng 1989, 28, 649–662.
  • El Awady, M. M. Natural Weathering, Artificial Photo-oxidation, and Thermal Aging of Low-Density Polyethylene: Grafting of Acrylic Acid onto Aged Polyethylene Films. J. Appl. Polym. Sci. 2003, 87, 2365–2237.
  • Barany, T.; Czigany, T.; Karger-Kocsis, J. Essential Work of Fracture Concept in Polymers. Periodica. Polytechnica. Ser. Mech. Eng 2003, 47, 91–102.
  • Wu, J.; Mai, Y.-W. The Essential Fracture Work Concept for Toughness Measurement of Ductile Polymers. Polym. Eng. Sci. 1996, 36, 2275–2288.
  • Maspoch, M. L.; Hénault, V.; Ferrer-Balas, D.; Velasco, J. I.; Santana, O. O. Essential Work of Fracture on PET Films: Influence of the Thickness and the Orientation. Polym. Test 2000, 19, 559–568.
  • Gupta, P.; Wilkes, G. L.; Sukhadia, A. M.; Krishnaswamy, R. K.; Lamborn, M. J.; Wharry, S. M.; Tso, C. C.; Deslauriers, P. J.; Mansfield, T.; Beyer, F. L. Does the Length of the Short Chain Branch Affect the Mechanical Properties of Linear Low-density Polyethylene? An Investigation Based on Films of Copolymers of Ethylene/1-butene, ethylene/1-hexene and Ethylene/1-octene Synthesized by a Single Site Metallocene Catalyst. Polymer 2005, 46, 8819–8837.
  • Fung, K. L.; Zhao, H. X.; Wang, J. T.; Meng, Y. Z.; Tjong, S. C.; Li, R. K. Y. Essential Work of Fracture (EWF) analysis for Compression Molded Alternating Poly (propylene Carbonate). Polym. Eng. Sci. 2004, 44, 580–587.
  • Fasce, L.; Chiaverano, G.; Lach, R.; Frontini, P. Essential Work of Fracture of Photo-oxidized LDPE/EVA Films. Macromol. Symp. 2007, 247, 271–281.
  • Casellas, J. J.; Frontini, P. M.; Carella, J. M. Fracture Characterization of Low-density Polyethylenes by the Essential Work of Fracture: Changes Induced by Thermal Treatments and Testing Temperature. J. Appl. Polym. Sci. 1999, 74, 781–796.
  • Karger-Kocsis, J.; Barany, T. Plane-stress Fracture Behavior of Syndiotactic Polypropylenes of Various Crystallinity as Assessed by the Essential Work of Fracture Method. Polym. Eng. Sci. 2002, 42, 1410–1419.
  • Hiver, J. M.; Etienne, J.; G’sell, C. Photomécanique, Etude par comportement des matériaux et des structures, April 24–26, Ed. Com’Science, 2001, 135–142, Poitiers, France.
  • Chabira, S. F.; Sebaa, M.; G’sell, C. Oxidation and Crosslinking Processes during Thermal Aging of Low-density Polyethylene Films. J Appl. Polym. Sci. 2012, 124, 5200–5208.
  • Kupper, L.; Gulmine, J. V.; Janissek, P. R.; Heise, H. M. Attenuated Total Reflection Infrared Spectroscopy for Micro-domain Analysis of Polyethylene Samples after Accelerated Ageing within Weathering Chambers. Vibrat. Spect. 2004, 34, 63–72.
  • Coates, J. Interpretation of Infrared Spectra, A Practical Approach. In Encyclopedia of Analytical Chemistry; R. A.Meyers, Ed.; Ó John Wiley & Sons Ltd: Chichester, 2000;10815–10837.
  • Carrasco, F.; Pagès, P.; Pascual, S.; Colom, X. Artificial Aging of High-density Polyethylene by Ultraviolet Irradiation. Eur. Polym. J. 2001, 37, 1457–1464.
  • Gulmine, J. V.; Akcelrud, L. FTIR Characterization of Aged XLPE. Polym. Test 2006, 25, 932–942.
  • Severini, F.; Gallo, R.; Ipsale, S.; Del Fanti, N. Environmental Degradation of Stabilized LDPE. Initial Step. Polym. Degrad. Stab 1986, 14, 341–350.
  • Borovanska, I.; Krastev, R.; Benavente, R.; Monleon Pradas, M.; s.; Lluch, A. V.; Samichkov, V.; Iliev, M. Ageing Effect on Morphology, thermal and Mechanical Properties of Impact Modified LDPE/PP Blends from Virgin and Recycled Materials. J. Elastom. Plast 2014, 46, 427–447.
  • Briassoulis, D.; Aristopoulou, A.; Bonora, M.; Verlodt, I. Degradation Characterization of Agricultural Low-density Polyethylene Films. Biosyst. Eng 2004, 88, 131–143.
  • Addiego, F.; Dahoun, A.; G'Sell, C.; Hiver, J.-M. Characterization of Volume Strain at Large Deformation under Uniaxial Tension in High-density Polyethylene. Polymer 2006, 47, 4387–4399.
  • Musuc, A. M.; Badea-Doni, M.; Jecu, L.; Rusu, A.; Popa, V. T. FTIR, XRD, and DSC Analysis of the Rosemary Extract Effect on Polyethylene Structure and Biodegradability. J. Therm. Anal. Calorim. 2013, 114, 169–177.
  • Chabira, S. F.; Sebaa, M.; Huchon, R.; De Jeso, B. The Changing Anisotropy Character of Weathered Low-density Polyethylene Films Recognized by Quasi-static and Ultrasonic Mechanical Testing. Polym. Degrad. Stab 2006, 91, 1887–1895.
  • Shahin, M. M.; Olley, R. H.; Blissett, M. J. Refinement of Etching Techniques to Reveal Lamellar Profiles in Polyethylene Banded Spherulites. J. Polym. Sci. B Polym. Phys. 1999, 37, 2279–2286.
  • Grabmayer, K.; Wallner, G. M.; Beißmann, S.; Braun, U.; Steffen, R.; Nitsche, D.; Roder, B.; Buchberger, W.; Lang, R. W. Accelerated Aging of Polyethylene Materials at High Oxygen Pressure Characterized by Photoluminescence Spectroscopy and Established Aging Characterization Methods. Polym. Degrad. Stab 2014, 109, 40–49.
  • Sugimoto, M.; Shimada, A.; Kudoh, H.; Tamura, K.; Seguchi, T. Product Analysis for Polyethylene Degradation by Radiation and Thermal Ageing. Radiat. Phys. Chem 2013, 82, 69–73.
  • La Mantia, F. P. Natural Weathering of Low Density polyethylene -III. Eur. Polvm. J 1984, 20, 993–995.
  • Martinez, A. B.; Gamez-Perez, J.; Sanchez-Soto, M.; Velasco, J. I.; Santana, O. O.; Maspoch, M. L. The Essential Work of Fracture (EWF) Method–Analyzing the Post-yielding Fracture Mechanics of Polymers. Eng. Fail. Anal 2009, 16, 2604–2617.
  • Martinez, A. B.; Segovia, A.; Gamez-Perez, J.; Maspoch, M. L. Essential Work of Fracture Analysis of the Tearing of a Ductile Polymer Film. Eng. Fract. Mech 2010, 77, 2654–2661.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.