References
- Mellin P, Björnberg O, Bengtsson I, et al. Proposed Swedish National Standard and best practice for detection of Ar In PM HIP material. Proceedings of the Euro PM2018 Congress & Exhibition; 2018; Bilbao, Spain.
- Broeckmann C. Toughness of duplex steel produced by PM-HIP. Mater Res Proc. 2019;10:169–181. doi:https://doi.org/10.21741/9781644900031-23
- Schaak C, Tillmann W, Schaper M, et al. Process gas infiltration in Inconel 718 samples during SLM processing. RTeJ Fachforum für Rapid Technol. 2016;2016(13).
- Tillmann W, Schaak C, Nellesen J, et al. Hot isostatic pressing of IN718 components manufactured by selective laser melting. Addit Manuf. 2016;13, doi:https://doi.org/10.1016/j.addma.2016.11.006
- Li P, Warner DH, Pegues JW, et al. Investigation of the mechanisms by which hot isostatic pressing improves the fatigue performance of powder bed fused Ti-6Al-4V. Int J Fatigue. 2019;120:342–352. doi:https://doi.org/10.1016/j.ijfatigue.2018.10.015
- Atkinson HV, Davies S. Fundamental aspects of hot isostatic pressing: an overview. Metall Mater Trans A. 2000;31(12):2981–3000. doi:https://doi.org/10.1007/s11661-000-0078-2
- National Research Council. Superalloys from powder: production and properties. Washington (DC): The National Academies Press; 1981. doi:https://doi.org/10.17226/19734
- Rashidi M, Liljestrand F, Eklund A, et al. Porosity regrowth during heat treatment of hot isostatically pressed additively manufactured IN718. Presentation During Euromat 2019, The European Congress and Exhibition on Advanced Materials and Processes, Stockholm, Sweden; 2019.