Ultraviolet‐filtered lighting and cellulose degradation: Evaluating the effect of light exposure on ethnographic collections

&
Pages 3-12 | Published online: 17 Sep 2010

References

  • Ali , M , Emsley , A M , Herman , H and Heywood , R J . 2001 . Spectroscopic studies of the ageing of cellulosic paper . Polymer , 42 : 2893 – 900 .
  • Ashley‐Smith , J , Derbyshire , A and Pretzel , B . The continuing development of a practical lighting policy for works of art on paper and other object types at the Victoria and Albert Museum . ICOM‐CC Preprints 13th Triennial Meeting Rio de Janeiro . Edited by: Vontobel , R. Vol. 1 , pp. 3 – 8 . London : James and James Ltd .
  • ASTM . 1997a . “ D919–92a standard test method for copper number of paper and paperboard. (Reapproved 1996, same as TAPPI T430m‐52) ” . In Annual Book of ASTM Standards , Edited by: ASTM . 121 – 3 . West Conshohocken : American Society for Testing and Materials .
  • ASTM . 1997b . “ D1926–95 standard test methods for carboxyl content of cellulose ” . In Annual Book of ASTM Standards , Edited by: ASTM . 391 – 3 . West Conshohocken : American Society for Testing and Materials .
  • Blair , H S and Cromie , R . 1977 . Spectroscopic investigation of some derivatives of oxycellulose in cadoxen solution . Journal of Applied Chemistry and Biotechnology , 27 : 205 – 13 .
  • Bradley , S. 1995 . “ The effect of light on ethnographic material ” . In Where to Start, Where to Stop? Papers from the British Museum/MEG Ethnographic Conservation Colloquium in Memory of Harold Gowers, London 9–10 November 1989 , Museum Ethnographers Group Occasional Papers Number 4 Edited by: Hill , L and Giles , S. 69 – 72 . Hull : Museum Ethnographers Group .
  • Bukovsky , V. 2000 . The natural ageing of paper after exposure to daylight . Restaurator , 21 : 229 – 37 .
  • Daniels , V. 1997 . The Conservation and Deterioration of Black Dyed New Zealand Flax. Part 1: The Degradation Mechanism , Conservation Research Group Internal Report 1997/5 London : British Museum Department of Conservation .
  • Daniels , V and McIntyre , I . An apparatus for studying conservation light bleaching . Conservation Science in the UK. Preprints of the Meeting held in Glasgow . Edited by: Tennent , N. May . pp. 122 – 4 . London : James and James Ltd . 1993
  • Ermolenko , I N and Savastenko , G N . 1966 . Microdetermination of carbonyl groups in cellulose materials by means of p‐nitrophenylhydrazine using diffuse reflectance spectra . Journal of Analytical Chemistry of the USSR , 21 : 81 – 4 .
  • Feller , R L , Lee , S B and Curran , M . 1985 . Three fundamental aspects of cellulose deterioration. (Annotated bibliographies) . Art and Archaeology Technical Abstracts , 22 : 277 – 354 . Supplement
  • Havermans , J B G A . 1995 . Environmental Influences on the Deterioration of Paper , Rotterdam : Barjesteh, Meeuwes & Co .
  • Havermans , J B G A and Dufour , J . 1997 . Photo oxidation of paper documents; a literature review . Restaurator , 18 : 103 – 14 .
  • HSE . 2002 . “ Control of Substances Hazardous to Health: The Control of Substances Hazardous to Health Regulations 2002 ” . In Approved Codes of Practice and Guidance, edn , 4th , London : Health and Safety Executive Books .
  • Lee , S B , Bogaard , J and Feller , R L . 1989 . Darkening of paper following exposure to visible and near‐ultraviolet radiation . Journal of the American Institute for Conservation , 28 : 1 – 18 .
  • Luo , M R , Cui , G and Rigg , B . 2001 . The development of the CIE 2000 colour‐difference formula: CIEDE2000 . Colour Research and Application , 26 : 340 – 50 .
  • McDonald , R and Smith , K J . 1995 . CIE94 ‐ a new colour‐difference formula . Journal of the Society of Dyers and Colourists , 111 : 376 – 9 .
  • McLaren , K and Rigg , B . 1976 . The SDC recommended colour‐difference formula: change to CIELAB . Journal of the Society of Dyers and Colourists , 92 : 337 – 8 .
  • Margutti , S , Conio , G , Calvini , P and Pedemonte , E . 2001 . Hydrolytic and oxidative degradation of paper . Restaurator , 22 : 67 – 83 .
  • Pretzel , B. Determining the colour fastness of the Bullerswood Carpet . Tradition and Innovation. Preprints IIC Melbourne Congress . Edited by: Roy , A. and Smith , P. pp. 150 – 4 . London : International Institute for Conservation .
  • Saunders , D and Kirby , J . Light‐induced damage: investigating the reciprocity principle . Preprints to the 11th /COM Committee for Conservation (ICOM‐CC) Triennial Meeting . September 1–6 1996 , Edinburgh. Edited by: Bridgland , J. Vol. 1 , pp. 87 – 90 . London : James and James Ltd .
  • Smith , C D and Wise , J K . 1967 . Infrared spectrometric examination of paper. 1. Techniques and fiber composition . Analytical Chemistry , 39 : 1698 – 705 .
  • TAPPI . 1976 . TAPPI Standard T235 os‐76 Alkali Solubility of Pulp at 25°C , New York : Technical Association of Pulp and Paper Industry .
  • Thomson , G. 1986 . The Museum Environment, edn , 2nd , Oxford : Butterworth‐Heinemann .
  • Whitmore , P M and Bogaard , J . 1994 . Determination of the cellulose scission route in the hydrolytic and oxidative degradation of paper . Restaurators , : 26 – 45 .
  • Zhbankov , R G . 1966 . Infrared Spectra of Cellulose and Its Derivatives , New York : Consultants Bureau .
  • Zou , X , Gurnagul , N , Uesaka , T and Bouchard , J . 1994 . Accelerated aging of papers of pure cellulose: mechanism of cellulose degradation and paper embrittlement . Polymer Degradation and Stability , 43 : 393 – 402 .
  • Author for correspondence.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.