Producing magnetite concentrate from iron tailings via suspension magnetization roasting: A pilot-scale study

, , &
Pages 1372-1382 | Received 18 Oct 2022, Accepted 16 Feb 2023, Published online: 16 Mar 2023

References

  • Zhang, X.; Gu, X.; Han, Y.; Parra-Álvarez, N.; Claremboux, V.; Kawatra, S. K. Flotation of Iron Ores: A Review. Min. Proc. Ext. Met. Rev. 2019, 42(3), 184–212. DOI: 10.1080/08827508.2019.1689494.
  • Singh, S.; Sahoo, H.; Rath, S. S.; Sahu, A. K.; Das, B. Recovery of Iron Minerals from Indian Iron Ore Slimes Using Colloidal Magnetic Coating. Powder Technol. 2015, 269, 38–45. DOI: 10.1016/j.powtec.2014.08.065.
  • Tang, Z. D.; Gao, P.; Li, Y. J.; Han, Y. X.; Li, W. B.; Butt, S.; Zhang, Y. H. Recovery of Iron from Hazardous Tailings Using Fluidized Roasting Coupling Technology. Powder Technol. 2020, 361, 591–599. DOI: 10.1016/j.powtec.2019.11.074.
  • Sun, Y. S.; Zhang, Q.; Han, Y. X.; Gao, P.; Li, G. F. Comprehensive Utilization of Iron and Phosphorus from High-Phosphorus Refractory Iron Ore. Jom-Us. 2018, 70(2), 144–149. DOI: 10.1007/s11837-017-2637-7.
  • Zhu, X. R.; Han, Y. X.; Sun, Y. S.; Li, Y. J.; Wang, H. W. Siderite as a Novel Reductant for Clean Utilization of Refractory Iron Ore. J. Clean. Prod. 2020, 245, 118704. DOI: 10.1016/j.jclepro.2019.118704.
  • Qi, C.; Fourie, A. Cemented Paste Backfill for Mineral Tailings Management: Review and Future Perspectives. Miner. Eng. 2019, 144, 144. DOI: 10.1016/j.mineng.2019.106025.
  • Roy, S. K.; Nayak, D.; Rath, S. S. A Review on the Enrichment of Iron Values of Low-Grade Iron Ore Resources Using Reduction Roasting-Magnetic Separation. Powder Technol. 2020, 367, 796–808. DOI: 10.1016/j.powtec.2020.04.047.
  • Wang, C.; Harbottle, D.; Liu, Q. X.; Xu, Z. H. Current State of Fine Mineral Tailings Treatment: A Critical Review on Theory and Practice. Miner. Eng. 2014, 58, 113–131. DOI: 10.1016/j.mineng.2014.01.018.
  • Fu, P. F.; Li, Z. Y.; Feng, J.; Bian, Z. Z. Recovery of Gold and Iron from Cyanide Tailings with a Combined Direct Reduction Roasting and Leaching Process. Metals-Basel. 2018, 8(7), 561. DOI: 10.3390/met8070561.
  • Bai, S. -J.; C-L, L.; X-Y, F.; Lv, C.; Wen, S. -M. Novel Method for Iron Recovery from Hazardous Iron Ore Tailing with Induced Carbothermic Reduction-Magnetic Flocculation Separation. Clean Technol. Environ. Policy. 2018, 20(4), 825–837. DOI: 10.1007/s10098-018-1501-y.
  • Bing, L.; Zhongying, Z.; Biao, T.; Hongbo, L.; Hanchi, C.; Zhen, M. (2018) Comprehensive Utilization of Iron Tailings in China. IOP Conference Series: Earth and Environmental Science 199. doi:10.1088/1755-1315/199/4/042055
  • Yuan, S.; Zhang, Q.; Yin, H.; Li, Y. Efficient Iron Recovery from Iron Tailings Using Advanced Suspension Reduction Technology: A Study of Reaction Kinetics, Phase Transformation, and Structure Evolution. J. Hazard. Mater. 2021, 404(Pt B), 124067. DOI: 10.1016/j.jhazmat.2020.124067.
  • Chu, C.; Deng, Y.; Zhou, A.; Feng, Q.; Ye, H.; Zha, F. Backfilling Performance of Mixtures of Dredged River Sediment and Iron Tailing Slag Stabilized by Calcium Carbide Slag in Mine Goaf. Constr. Build. Mater. 2018, 189, 849–856. DOI: 10.1016/j.conbuildmat.2018.09.049.
  • Gayana, B. C.; Chandar, K. R. Sustainable Use of Mine Waste and Tailings with Suitable Admixture as Aggregates in Concrete Pavements-A Review. Adv Concr Constr. 2018, 6(3), 221–243. DOI: 10.12989/acc.2018.6.3.221.
  • da Silva Fl; Araújo, F. G. S.; Teixeira, M. P.; Gomes, R. C.; von Krüger Fl. Study of the Recovery and Recycling of Tailings from the Concentration of Iron Ore for the Production of Ceramic. Ceram. Int. 2014, 40(10), 16085–16089. DOI: 10.1016/j.ceramint.2014.07.145.
  • Li, S.; Guo, Z.; Pan, J.; Zhu, D.; Dong, T.; Lu, S. Stepwise Utilization Process to Recover Valuable Components from Copper Slag. Minerals. 2021, 11(2). DOI: 10.3390/min11020211.
  • Pandiri, S.; Raju, M. V.; Harikrishna, M.; Bonda, R.; Saha, R.; Attel, U. Enhanced Iron Recovery from Ultrafine Iron Ore Tailing Through Combined Gravitational and Magnetic Separation Process. T. Indian I. Metals. 2022, 75(9), 2435–2442. DOI: 10.1007/s12666-022-02621-6.
  • Araujo, V. A.; Lima, N.; Azevedo, A.; Bicalho, L.; Rubio, J. Column Reverse Rougher Flotation of Iron Bearing Fine Tailings Assisted by HIC and a New Cationic Collector. Miner. Eng. 2020, 156, 156. DOI: 10.1016/j.mineng.2020.106531.
  • Panda, L.; Biswal, S. K.; Venugopal, R.; Mandre, N. R. Recovery of Ultra-Fine Iron Ore from Iron Ore Tailings. T. Indian I. Metals. 2017, 71(2), 463–468. DOI: 10.1007/s12666-017-1177-8.
  • Kumar, R.; Mandre, N. R. Characterization and Beneficiation of Iron Ore Tailings by Selective Flocculation. T. Indian I. Metals. 2015, 69(7), 1459–1466. DOI: 10.1007/s12666-015-0667-9.
  • Yu, J. W.; Han, Y. X.; Li, Y. J.; Gao, P. Recent Advances in Magnetization Roasting of Refractory Iron Ores: A Technological Review in the Past Decade. Min. Proc. Ext. Met. Rev. 2020, 41(5), 349–359. DOI: 10.1080/08827508.2019.1634565.
  • Boehm, A.; Boehm, M.; Kogelbauer, A. Neutrons for Mineral Processing - Thermo Diffractometry to Investigate Mineral Selective Magnetizing Flash Roasting. Chem. Ing. Tech. 2014, 86(6), 883–890. DOI: 10.1002/cite.201400024.
  • Yu, J. W.; Han, Y. X.; Li, Y. J.; Gao, P. Beneficiation of an Iron Ore Fines by Magnetization Roasting and Magnetic Separation. Int. J. Mineral Process. 2017, 168, 102–108. DOI: 10.1016/j.minpro.2017.09.012.
  • Zhang, Q.; Sun, Y. S.; Han, Y. X.; Li, Y. J.; Gao, P. Effect of Thermal Oxidation Pretreatment on the Magnetization Roasting and Separation of Refractory Iron Ore. Min. Proc. Ext. Met. Rev. 2020, 43(2), 182–187. DOI: 10.1080/08827508.2020.1837126.
  • Zhang, Q.; Sun, Y. S.; Han, Y. X.; Gao, P.; Li, Y. J. Thermal Decomposition Kinetics of Siderite Ore During Magnetization Roasting. Mining Metall Explor. 2021, 38(3), 1497–1508. DOI: 10.1007/s42461-021-00417-8.
  • Yu, D. W.; Utigard, T. A.; Barati, M. Fluidized Bed Selective Oxidation-Sulfation Roasting of Nickel Sulfide Concentrate: Part I. Oxidation Roasting. Metall Mater Trans B. 2014, 45(2), 653–661. DOI: 10.1007/s11663-013-9958-x.
  • Wang, J.; Wang, S. D.; Zhang, L.; Du, G. C.; He, W. Y. Industrial Application of Large Rotary Kiln for Recovery of Vanadium from Vanadium Slag Added MnVo4 in Calcium Roasting Process. ISIJ Int. 2017, 57(12), 2255–2262. DOI: 10.2355/isijinternational.ISIJINT-2017-097.
  • Li, Y. J.; Wang, R.; Han, Y. X.; Wei, X. C. Phase Transformation in Suspension Roasting of Oolitic Hematite Ore. J. Cent. South Univ. 2015, 22(12), 4560–4565. DOI: 10.1007/s11771-015-3006-8.
  • Jin, J.; Zhu, X.; Li, P.; Li, Y.; Han, Y. Clean Utilization of Limonite Ore by Suspension Magnetization Roasting Technology. Minerals. 2022, 12(2). DOI: 10.3390/min12020260.
  • Tang, Z.; Xiao, H.; Sun, Y.; Gao, P.; Zhang, Y. Exploration of Hydrogen-Based Suspension Magnetization Roasting for Refractory Iron Ore Towards a Carbon-Neutral Future: A Pilot-Scale Study. Int. J. Hydrogen Energy. 2022, 47(33), 15074–15083. DOI: 10.1016/j.ijhydene.2022.02.219.
  • Zhang, X. L.; Han, Y. X.; Sun, Y. S.; Li, Y. J. Innovative Utilization of Refractory Iron Ore via Suspension Magnetization Roasting: A Pilot-Scale Study. Powder Technol. 2019, 352, 16–24. DOI: 10.1016/j.powtec.2019.04.042.
  • Sun, Y. S.; Zhang, X. L.; Han, Y. X.; Li, Y. J. A New Approach for Recovering Iron from Iron Ore Tailings Using Suspension Magnetization Roasting: A Pilot-Scale Study. Powder Technol. 2020, 361, 571–580. DOI: 10.1016/j.powtec.2019.11.076.
  • Zeng, L.; Tong, A.; Kathe, M.; Bayham, S.; Fan, L. -S. Iron Oxide Looping for Natural Gas Conversion in a Countercurrent Moving Bed Reactor. Appl. Energy. 2015, 157, 338–347. DOI: 10.1016/j.apenergy.2015.06.029.
  • Tang, Z.; Zhang, Q.; Sun, Y.; Gao, P.; Han, Y. Prospects of Green Extraction of Iron from Waste Dumped Flotation Tailings by H2: A Pilot Case Study. J. Clean. Prod. 2022, 330, 330. DOI: 10.1016/j.jclepro.2021.129853.
  • Zhang, Q.; Sun, Y.; Han, Y.; Li, Y.; Gao, P. Producing Magnetite Concentrate via Self-Magnetization Roasting in N2 Atmosphere: Phase and Structure Transformation, and Extraction Kinetics. J. Ind. Eng. Chem. 2021, 104, 571–581. DOI: 10.1016/j.jiec.2021.09.008.
  • Yuan, S.; Liu, X.; Gao, P.; Han, Y. A Semi-Industrial Experiment of Suspension Magnetization Roasting Technology for Separation of Iron Minerals from Red Mud. J. Hazard. Mater. 2020, 394, 122579. DOI: 10.1016/j.jhazmat.2020.122579.
  • Jordán, D.; González-Chávez, D.; Laura, D.; León Hilario, L. M.; Monteblanco, E.; Gutarra, A.; Avilés-Félix, L. Detection of Magnetic Moment in Thin Films with a Home-Made Vibrating Sample Magnetometer. J. Magn. Magn. Mater. 2018, 456, 56–61. DOI: 10.1016/j.jmmm.2018.01.088.
  • Carmignano, O.; Vieira, S.; Teixeira, A. P.; Lameiras, F.; Brandão, P. R.; Lago, R. Iron Ore Tailings: Characterization and Applications. J. Braz. Chem. Soc. 2021. DOI: 10.21577/0103-5053.20210100.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.