Effect of the aspect ratio of the pre-existing rectangular adhesion failure on the structural integrity of the adhesively bonded single lap joint

ORCID Icon, &
Pages 2093-2111 | Received 14 Mar 2019, Accepted 31 May 2019, Published online: 26 Jun 2019

References

  • Karachalios EF, Adams RD, da Silva L. Single lap joints loaded in tension with high strength steel adherends. Int J Adhes Adhes. 2013;43:81–95.
  • Karachalios EF, Adams RD, Da Silva L. Strength of single lap joints with artificial defects. Int J Adhes Adhes. 2013;45:69–76.
  • Volkersen O. Die Nietkraftverteilung in zugbeanspruchten\mbox{Nietverbindungen} mit konstanten Laschenquerschnitten. Luftfahrtforschung. 1938;15:41–47.
  • Goland M, Reissner E. The stresses in cemented lap joints. Trans ASME, J Appl Mech. 1944;6611:A17–A27.
  • Hart-Smith LJ. Adhesive-bonded single-lap joints. Douglas Aircraft Co., NASA Langley report CR112236. 1973;1–114.
  • Adams RD, Peppiatt NA. Stress analysis of adhesive-bonded lap joints. J Strain Anal. 1974;9:185–196.
  • da Silva LFM, das Neves PJC, Adams RD, et al. Analytical models of adhesively bonded joints-Part II: Comparative study. Int J Adhes Adhes. 2009;29:331–341.
  • Panigrahi SK, Pradhan B. Adhesion failure propagation in adhesively-bonded single-lap laminated FRP composite joints. J Adhes Sci Technol. 2007;21:379–398.
  • Das RR, Pradhan B. Adhesion failure analyses of bonded tubular single lap joints in laminated fibre reinforced plastic composites. Int J Adhes Adhes. 2010;30:425–438.
  • Parida SK, Pradhan AK. Effect of material anisotropy on delamination damage in adhesive bonded lap shear joints made with curved laminated FRP composite panels. Iran J Sci Technol Trans Mech Eng. 2016;40:275–287.
  • Pradhan AK, Parida SK. 3D FE delamination induced damage analyses of adhesive bonded lap shear joints made with curved laminated FRP composite panels. J Adhes Sci Technol. 2013;27:1104–1121.
  • Raju IS, Crews JH, Aminpour MA. Convergence of strain energy release rate components for edge-delaminated composite laminates. Eng Fract Mech. 1988;30:383–396.
  • Tay T. Characterization and analysis of delamination fracture in composites: an overview of developments from 1990 to 2001. Appl Mech Rev. 2003;56:1.
  • Panigrahi SKP. Three dimensional failure analysis and damage propagation behavior of adhesively bonded single lap joints in laminated FRP composites. J Reinf Plast Comp. 2007;26:193–201.
  • Rybicki EF, Kanninen MF. A finite element calculation of stress intensity factors by a modified crack closure integral. Eng Fract Mech. 1977;9:931–938.
  • Krueger R. Virtual crack closure technique: History, approach, and applications. Appl Mech Rev. 2004;57:109.
  • Lee RJ, Butler JR, Yates T, Davidson R. MTS adhesives project 2 failure modes and criteria. Report No. 5: Anne 1– test methods for adhesive fracture properties. Department of Trade and Industry, AEA Technology, Harwell, Didcot, United Kingdom. 1997;1–26.
  • Tomczyk AJ. MTS adhesives project 2 failure modes and criteria. Report No. 5 – test methods for adhesive fracture properties overall summary. Department of Trade and Industry, AEA Technology, Harwell, Didcot, United Kingdom. 1997;1–23.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.