Copper release rate needed to inhibit fouling on the west coast of Sweden and control of copper release using zinc oxide

, , , , , , & show all
Pages 453-463 | Received 07 Dec 2017, Accepted 06 Apr 2018, Published online: 15 May 2018

References

  • Almeida E, Diamantino TC, de Sousa O. 2007. Marine paints: the particular case of antifouling paints. Prog Org Coat. 59:2–20. doi: 10.1016/j.porgcoat.2007.01.017.10.1016/j.porgcoat.2007.01.017
  • Andersson K, Brynolf S, Lindgren JF, Wilewska-Bien M. 2016. Shipping and the environment – improving environmental performance in marine transportation. Berlin-Heidelberg: Springer.
  • Bellotti N, Romagnoli R. 2014. Assessment of zinc salicylate as antifouling product for marine coatings. Ind Eng Chem Res. 53:14559–14564. doi: 10.1021/ie5015734.10.1021/ie5015734
  • Biggs TW, D’Anna H. 2012. Rapid increase in copper concentrations in a new marina, San Diego Bay. Mar Poll Bull. 64:627–635. doi: 10.1016/j.marpolbul.2011.12.006.10.1016/j.marpolbul.2011.12.006
  • Copper EU RAR. 2008. European Union risk assessmentreport: voluntary risk assessment of copper, copper II sulphate pentahydrate, copper(I) oxide, copper(II) oxide, dicopper chloride tri-hydroxide. Brussels: European Copper Institute. https://echa.europa.eu/sv/copper-voluntary-risk-assessment-reports.
  • Dahlstrom M, Elwing H, Ytreberg E, Soler C, Dahlstrom M. 2014. Bland borsttvättar och fartygsfärger - en studie av fritidsbåtsägares attityder till användning av olika antifoulingtekniker [Among boat washs and antifouling paints for commercial shipping – a study of leisure boaters attitudes towards different antifouling techniques]. CHANGE prestudy.
  • EU Parliament. 1998. Council Directive 98/8/EC of the European Parliament and of the council of 16 February, 1998. Concerning the placing of biocidal products on the market.
  • EU Parliament. 2000. Directive 2000/60/EC of the European parliament and of the council of 23 October 2000 establishing a framework for Community action in the field of water policy. Off J Eur Commun. 327/64.
  • Finnie A. 2006. Improved estimates of environmental copper release rates from antifouling products. Biofouling. 5:279–291. doi: 10.1080/08927010600898862.10.1080/08927010600898862
  • French MS, Evans LV, Dalley R. 1984. Raft trial experiment on leaching from antifouling paints. Trans Inst Mar Eng. 97:127–130.
  • Hellio C, Yebra DM. 2009. Advances in marine antifouling coatings and technologies. Amsterdam: Elsevier.10.1533/9781845696313
  • Hugget MJ, Nedved BT, Hadfield MG. 2009. Effects of initial surface wettability on biofilm formation and subsequent settlement of Hydroides elegans. Biofouling. 25:387–399. doi: 10.1080/08927010902823238.10.1080/08927010902823238
  • Hung OS, Thiyagarajan V, Qian PY. 2008. Preferential attachment of barnacle larvae to natural multi-species biofilms: does surface wettability matter? J Exp Mar Biol Ecol. 361:36–41. doi: 10.1016/j.jembe.2008.04.011.10.1016/j.jembe.2008.04.011
  • IMO. 2001. International convention on the control of harmful anti-fouling systems on ships. London.
  • IMO. 2005. Revised guidelines for the indentification and designation of particularly sensitive sea areas. London: IMO.
  • ISO. 2007. Determination of the release rate of biocides from anti-fouling paints International Standard ISO 15181:2007.
  • ISO. 2010. Modelling of biocide release rate from qntifouling paints by mass-balance calculation. International Standard ISO 10890:2010.
  • Jessop A, Turner A. 2011. Leaching of Cu and Zn from discarded boat paint particles into tap water and rain water. Chemosphere. 83:1575–1580. doi: 10.1016/j.chemosphere.2011.01.021.10.1016/j.chemosphere.2011.01.021
  • Jones B, Bolam T. 2007. Copper speciation survey from UK marinas, harbours and estuaries. Mar Poll Bull. 54:1127–1138.
  • Karlsson J, Ytreberg E, Eklund B. 2010. Toxicity of anti-fouling paints for use on ships and leisure boats to non-target organisms representing three trophic levels. Environ Pollut. 158:681–687. doi: 10.1016/j.envpol.2009.10.024.10.1016/j.envpol.2009.10.024
  • Kiil S, Dam-Johansen K, Weinell CE, Pedersen MS. 2002. Seawater-soluble pigments and their potential use in self-polishing antifouling paints: simulation-based screening tool. Prog Org Coat. 45:423–434. doi: 10.1016/S0300-9440(02)00146-7.10.1016/S0300-9440(02)00146-7
  • Kruskal WH, Wallis WA. 1952. Use of ranks in one-criterion variance analysis. J Am Stat Assoc. 47:583–621. doi: 10.1080/01621459.1952.10483441.10.1080/01621459.1952.10483441
  • Lagerqvist M, Andersson M. 2016. Båtlivsundersökningen [The Boating Investigation] 2015. Sweden: Gothenburg.
  • Lagerström ME, Lindgren JF, Holmqvist A, Dahlström M, Ytreberg Y. 2018. In situ release rates of Cu and Zn from commercial antifouling paints at different salinities. Mar Poll Bull. 127:289–296. doi: 10.1016/j.marpolbul.2017.12.027.10.1016/j.marpolbul.2017.12.027
  • Levene H 1960. Contributions to probability and statistics: essays in honor of Harold. Hotelling: Stanford University Press.
  • Manzo S, Buono S, Cremisini C. 2008. Predictability of copper, irgarol, and diuron combined effects on sea urchin Paracentrotus lividus. Arch Environ Contam Toxicol. 54:57–68. doi: 10.1007/s00244-007-9009-1.10.1007/s00244-007-9009-1
  • Olsen SM, Pedersen LT, Dam-Johansen K, Kristensen JB, Kiil S. 2010. Replacement of traditional seawater-soluble pigments by starch and hydrolytic enzymes in polishing antifouling coatings. J Coat Technol Res. 7:355–363. doi: 10.1007/s11998-009-9191-3.10.1007/s11998-009-9191-3
  • Schiff K, Diehl D, Valkirs A. 2004. Copper emissions from antifouling paint on recreational vessels. Mar Poll Bull. 371–377. doi: 10.1016/j.marpolbul.2003.08.016.10.1016/j.marpolbul.2003.08.016
  • Srinivasan M, Swain GW. 2007. Managing the use of copper-based antifouling paints. Environ Manage. 39:423–441. doi: 10.1007/s00267-005-0030-8.10.1007/s00267-005-0030-8
  • Thomas KV, Brooks S. 2010. The environmental fate and effects of antifouling paint biocides. Biofouling. 26:73–88. doi: 10.1080/08927010903216564.10.1080/08927010903216564
  • Turner A, Comber S, Rees AB, Gkiokas D, Solman K. 2015. Metals in boat paint fragments from slipways, repair facilities and abandoned vessels: an evaluation using field portable XRF. Talanta. 131:372–378. doi: 10.1016/j.talanta.2014.08.012.10.1016/j.talanta.2014.08.012
  • Valkirs AO, Seligman PF, Haslbeck E, Caso JS. 2003. Measurement of copper release rates from antifouling paint under laboratory and in situ conditions: implications for loading estimation to marine water bodies. Mar Poll Bull. 46:763–779. doi: 10.1016/S0025-326X(03)00044-4.10.1016/S0025-326X(03)00044-4
  • Voulvoulis N, Scrimshaw MD, Lester JN. 1999. Alternative antifouling biocides. Appl Organomet Chem. 13:135–143. doi: 10.1002/(ISSN)1099-0739.10.1002/(ISSN)1099-0739
  • Woods Hole Oceanographic Institution. 1952. Marine fouling and its prevention. Menasha: George Banta Publishing Co.
  • Yebra DM, Kiil S, Dam-Johansen K. 2004. Antifouling technology - past, present and future steps towards efficient and environmentally friendly antifouling coatings. Prog Org Coat. 50:75–104. doi: 10.1016/j.porgcoat.2003.06.001.10.1016/j.porgcoat.2003.06.001
  • Yebra DM, Kiil S, Weinell CE, Dam-Johansen K. 2006. Dissolution rate measurements of sea water soluble pigments for antifouling paints: ZnO. Prog Org Coat. 56:327–337. doi: 10.1016/j.porgcoat.2006.06.007.10.1016/j.porgcoat.2006.06.007
  • Ytreberg E 2012. Dispersion of biocides from boats - investigation of different sources and their contribution. [Spridning av biocider från båtar-Undersökning av olika källor och dess bidrag]. Department of Applied Environmental Science, Stockholm university.
  • Ytreberg E, Lundgren L, Bighiu MA, Eklund B. 2015. New analytical application for metal determination in antifouling paints. Talanta. 143:121–126. doi: 10.1016/j.talanta.2015.05.001.10.1016/j.talanta.2015.05.001
  • Ytreberg E, Lagerström M, Holmquist A, Eklund B, Elwing H, Dahlström M, Dahl P, Dahlström M. 2017. A novel XRF method to measure environmental release of copper and zinc from antifouling paints. Environ Poll. 225:490–496. doi: 10.1016/j.envpol.2017.03.014.10.1016/j.envpol.2017.03.014
  • Zinc EU RAR. 2010. European Union risk assessment report zinc metal. Luxembourg: Office for Official Publications of the European Communities. http://publications.jrc.ec.europa.eu/repository/handle/JRC61245.