- Costa JM, Ferreira JM, Capela C. Fracture toughness of the heat affected zone on Nd-YAG laser welded joints. Eng Fail Anal. 2008;6:93.
- Chavanne RL. Forty-four ways to improve the hardfacing operation. Weld J. 1999;62:15.
- Dasa D, Duttab AK, Rayc KK. Influence of varied cryo-treatment on the wear behaviour of AISI D2 steel. Wear J. 2008;31:297–309.
- Borrego LP, Pires JTB. Mould steels repaired by laser welding. Eng Fail Anal. 2008;8:596–607.
- Saaedi J, Coyle TW, Mirdamadi S, et al. Phase formation in a Ni–50Cr HVOF coating. Surf Coat Technol. 2008;202(24):5804–5811.
- Karthikeyan J, Berndt CC, Reddy S, et al. Nanomaterial deposts formed by DC plasma spraying of liquid feedstocks. Weld J. 1998;81:121.
- Losano G, Morgenfeld J. Criteria for assessing the risk of cracking when hot working. Revista Soldadura. 2001;4(11):326–327.
- Lin YC, Wang SW, Wu KE. The wear behaviour of machine tool guideways clad with W-Ni, W-Co and W-Cu using gas tungsten arc welding. Surf Coat Technol. 2003;172(2–3):158–165.
- Geng Z, Li S, Duan DL, et al. Wear behaviour of WC-Co HVOF coatings at different temperatures in air and argon. Wear. 2015;330–331:348–353.