26
Views
5
CrossRef citations to date
0
Altmetric
Original Articles

Corrosion failure and its prevention in light water reactor power plants

Pages 209-216 | Published online: 05 Jan 2010

References

  • Bush , S H and Dillon , R L . 1977 . ‘Stress corrosion cracking and hydrogen embrittlement of iron base alloys.’ , Edited by: Staehle , R W . 61 NACE . NACE-5
  • Cheng , C F . 1975 . J Nucl Mater , 56 : 11
  • EPRI . . pp. 4 Chicago meeting March
  • EPRI . . Compilation of information from BWR pipe cracking meeting. Chicago May
  • Copeland , J F and Giannuzzi , A J . 1984 . ‘Long-term integrity of nuclear power plant components.’ EPRI NP-3673–LD Project 2057–4 Final Report October
  • Japan Welding Engineering Society . 1978 . ‘Tests and studies on local structural movements and safety assessments for reactor pipework systems (Part 3).’ JWES AE-7807
  • Uchida . 1987 . Nuclear Industry , 33 ( 4 ) : 15
  • Akaishi . 1980 . Corrosion-proofing Techniques , 29 : 142
  • Mukai , Murata and Sakai . Lecture resume of the Japan Welding Society National Conference 1987 (40) 176
  • ASME Boiler and Pressure Vessel Code Section III 1977
  • Kume . 1977 . The Japan Welding Society lecture resume , 62 ( 20 )
  • Miki . 1978 . Hitachi Review , 60 ( 13 )
  • Umemoto and Tanaka . 1978 . Ishikawa-jima Harima Technical Report , 18 : 29
  • Ford , F P and Povich , M J . 1979 . Corrosion , 35 : 569
  • Danco , J C and Indig , M E . 1982 . ‘Predictive method for assessing corrosion damage to BWR piping and PWR steam generators.’ . NACE , : 112
  • Indig , M E and Weber , J E . 1985 . Corrosion , 41 : 170
  • Indig , M E . Paper presented to seminar on ‘Countermeasures for BWR pipe cracking’ Palo Alto, January 1980
  • Spiewak , I , Livingston , R S and Negin , C A . 1985 . EPRI NP 4208
  • Kikuchi , Onaka and Minato . 1984 . Corrosion Resistance Techniques , 33 : 33
  • Tatone , O S , Meindal , P and Taylor , G F . 1986 . ‘Steam generator tube performance. Experience with water-cooled nuclear power reactors during 1983 and 1984.’ AECL-9107
  • Green , S J and Paine , J PN . 1981 . Nucl Tech , 55 ( 10 )
  • Coriou , H . 1966 . Corrosion , 22 : 280
  • Weeks , J R . 1976 . Nucl Tech , 28 : 348
  • Blale , F M . 1982 . Nucl News , December : 49
  • Sedricks , A J . 1979 . Corrosion-proofing Techniques , 28 : 82
  • Fletcher , W D and Malinowski , D D . 1976 . Nucl Tech , 28 : 356
  • Weeks , J R . 1974 . ‘Corrosion problems in energy conversion and generation.’ , 322 The Electrochem Soc Inc .
  • Panson , A J . 1975 . J Electrochem Soc , 122 : 915
  • Pettit , P J and Mctique , P F . 1978 . Mater Perform , 17 : 36
  • Airey , G P and Pement , F W . 1983 . Corrosion , 39 : 46
  • Bandy , R , Roberge , R and Van Rooyen , D . April 1984 . ‘Corrosion 1984’ April , Paper No. 179
  • Mirglin , B P and Sarver , L W . March 1985 . ‘Corrosion 1985’ March , Paper No.89
  • Nagano , H , Tokimasa , K , Yamanaka , K and Miyuki , H . 1985 . ‘Effect of environmental and material factors on the intergranular attack of alloy 600.’ EPRI workshop on ‘Remedial actions for secondary side intergranular corrosion.’ October
  • Scott , P M . 1985 . Corros Sci , 25 : 583
  • 1962 . Zirconium data manual UKAEA TRG Report 108R
  • Urquhart , A W . 1918 . J Electrochem Soc , 125 : 199
  • Kuwae , R . 1983 . J Nucl Mater , 119 : 229
  • Ramasubramanian , N . 1983 . J Nucl Mater , 119 : 208
  • Gazzarolli , K . June-July 1977 . ‘KWU observations and hypothesis of PCI failure.’ June-July , Vienna IAEA specialists
  • Juncrans and Varnild , O . ASEA-ATOM research on PCI, ANS topical meeting, St Charles, May 1977
  • Penn , W J . 1977 . Nucl Tech , 34 : 249
  • Ichikawa . 1976 . Nuclear Industry , 24 ( 9 ) : 17
  • Ishihara and Obashi . ‘Corrosion/Anti-corrosion 1986’ the collection of pre-drafts for lectures, A306 1986 105
  • Fukuda and Akaishi . Collection of pre-drafts for No.33 corrosion/anti-corrosion discussion A-110 1986 43
  • Kuniya , Sugano , Masaoka and Sasaki . 1983 . Corrosion-proofing Techniques , 32 : 649
  • Kalderon , D . 1972 . Proc Inst Mech Engrs , 186 : 379
  • Vyas , B . 1981 . Nucl Tech , 55 : 525
  • Kondo . 1977 . J of the Japan Material Strength Society , 14 : 141

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.