References
- Ogawa , T , Sakaguchi , J , Kobayashi , T and Ando , Y . 26–28 Oct 1986 . “ ‘Development of duplex stainless steel line pipe.’ ” . In Preprint of International conference on ‘Duplex stainless steel’ 26–28 Oct , 77082 the HAgue
- Eckstein , H H and Viehrih , H W . 1982 . ‘Contribution to the transformation behaviour of ferritic-austenitic chromium-nickel steels taking particular account of welding-decomposition behaviour.’ . Neue Hutte (Leipzig) , 27 ( 11 ) : 409 – 414 .
- Wehner , H and Speckhardt , H . 1979 . ‘Precipitation and corrosion behaviour of a ferritic-austenitic chromium-nickel-molybdenum steel after brief annealing taking particular account of welding.’ . Z Werkst-Techn, (Weinheim) , 10 : 317 – 332 .
- Tosch , J , Rabensteiner , G and Reitere , P . ‘Metallurgy of the welding of corrosion resistant ferritic-austenitic CrNiMoN alloy steels (duplex steels).’ . Berg-u Huttenm Mh , 132 ( 5 ) 147 – 154 .
- Rabensteiner , G , Tosch , J and Schabereiter , H . 1980 . ‘Hot cracking tests on chemically resistant weld metal deposits with the recently developed PVR test.’ . Schweisstechnik (Vienna) , 34 ( 12 ) : 213 – 217 .
- Espy , R H . 1982 . ‘Weldability of nitrogen-strengthened stainless steels.’ . Weld J (New York) , 61 ( 5 ) : 149s – 156s .