- Ishihara , Shimizu and Ito . 1973 . ‘Stress corrosion cracking induced by high‐temperature water in reinforced weld metal of austenitic stainless steels’ . J Jpn Weld Soc , 37 (11) : 1217 – 1223 .
- Nakao and Nishimoto . 1986 . ‘Microstructure of austenitic stainless steel weld metal and factors controlling pitting corrosion resistance’ . Proc 67 ‘Corrosion protection’ symposium . 1986 . pp. 1 – 10 .
- Devine , T M . 1980 . ‘Influence of carbon content and ferrite morphology on the sensitisation of duplex stainless steel’ . Met Trans A , IIA (5) : 791 – 800 .
- Makishima , K. 1960 . ‘Quantitative morphology’ , Uchida Press .
- Ikawa , Nakao , Nishimoto and Inoue . 1978 . ‘Investigation of SUS304 weld decay (1st report)’ . J Jpn Weld Soc , 47 (5) : 252 – 259 .
- Hasegawa , M . 1974 . ‘Introduction to stainless steels’ 222
- Nakao and Nishimoto . 1987 . ‘Surface sensitisation treatment of stainless steels by laser’ . Quart JJpn WeldSoc , 5 (4) : 445 – 451 .
- Tedmon , C S . 1971 . ‘Intergranular corrosion of austenitic stainless steel’ . J Electrochem Soc , 118 (2) : 192 – 202 .
- Stawstrom , C S and Hillert , M . 1969 . ‘An improved depleted‐zone theory of intergranular corrosion of 18–8 stainless steel’ . JISI , 207 : 77 – 85 .
- Wolf , R A and Paxton , H W . 1963 . Trans Met Soc AIME , 230 : 1426