413
Views
30
CrossRef citations to date
0
Altmetric
TECHNICAL NOTE

Spurious Mild Wear Measurement Using White Light Interference Microscopy in the Presence of Antiwear Films

, , &
Pages 841-846 | Received 09 Jul 2009, Accepted 12 Jul 2009, Published online: 30 Oct 2009

REFERENCES

  • Tasan , Y. C. , de Rooij , M. B. and Schipper , D. J. 2005 . “Measurement of Wear on Asperity Level Using Image-Processing Techniques,” . Wear , 258 : 83 – 91 .
  • Spikes , H. A. 2004 . “The History and Mechanisms of ZDDP,” . Trib. Lett. , 17 : 465 – 485 .
  • Topolovec-Miklozic , K. , Forbus , T. R. and Spikes , H. A. 2007 . “Film Thickness and Roughness of ZDDP Antiwear Films,” . Trib Lett. , 26 : 161 – 171 .
  • Topolovec-Miklozic , K. , Forbus , T. R. and Spikes , H. A. 2008 . “The Film-Forming and Friction Properties of Overbased Calcium Sulphonate Detergents,” . Trib. Lett. , 29 : 33 – 44 .

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.