References
- Shi Erwei, et al., Hydrothermal Crystallization, Science Press 30, (2004).
- B. Hao, K. Fang, and L. Xiang. Effect of Precursor on aggregation of AlOOH nono-particles prepared by hydrothermal process. China Powder Science and Technology 15, 68–71 (2009).
- B. Hao, 173 L. Xiang, and K. Fang. Effect of the Saturation on the Nano-AlOOH hydrothermal crystal morphology. New Technology & New Process 11, 109–111 (2009).
- B. Hao, K. Fang, and L. Xiang. Hydrothermal crystallization mechanism and the interface model of nano-AlOOH in different kinds of pH media. collection of theses from the 9th China Particle Preparation and Treatment Seminar [C]Shandong: Professional Committee of Particle Preparation and Treatment. Chinese Society of Particuology, 10, 105–109 (2009).
- B. Hao, K. Fang, and L. Xiang. Hydrothermal crystallizaton mechanism and growth unit model of nano-scale γ -AlOOH. Chemical Engineering Magazine 38(1), 71–74 (2010).
- S.C. Kuiry, E. Megen, S.D. Patil, et al., Solution-based synthesis of boehmite nanofibers and alumina nanorods. Journal of Physical Chemistry B 109(9), 3868–3872 (2005).
- H.D. S. Santos, P.K. Kiyohara, and P.D. S. Santos. Thermal transformation of synthetic euhedral and fibrillar crystals of boehmite into alumina. Material Research Bulletin 31, 799–807 (1996).
- H.Y. Zhu, J.D. Riches, and J.C. Barry. Alumina nanofibers prepared from aluminum hydrate with poly (ethylene oxide) Surfactant. Chemistry of Materials 14, 2086–2093 (2002).
- R.S. Doremus, B.W. Roberts, and D. Turnbull. Growth and perfection of crystals. Cooper-stown Conference, 56–74 (1958).
- R.S. Wangner, and W.C. Ellis. The VLS mechanism of whisker growth. Trans.Met.Soc.Aime 233, 1054–1064 (1986).
- G.W. Sears, Screw dislocation theory of whisker growth. Acta Met 1, 457–459 (1953).
- Y.F. Li, C.D. Qin, and D.H. L. Ng. Morphology and growth mechanism of alumina whiskers in aluminum-basedmetalmatrix composites. Journal ofMaterials Research 14, 2997–3000 (1999).
- L. Xiang, Y. Wen, Q. Wang, and Y. Jin. Formation and characterization of dispersive mg substituted CaCO3. Materials Letters 60, 1719–1723 (2006).
- R. Kiessling. The influence of non-metallic inclusion on the properties of steel. J. of Metals, 197, 48–54 (1969).
- S. Malm. On the precipitation of slag inclusions during solidification of high-carbon steel, deoxidized with aluminium and mish metal. scand. J.of Metall 15, 248–257 (1976).
- S. Rudnik. Discontinuities in hot-rolled steel caused by non-metallic inclusion. JISI 204(4), 374–376 (1966).