Influence of Silicon Carbide/Graphite addition on properties of AA6082 reinforced composites

, , , , ORCID Icon &
Pages S176-S184 | Received 19 Sep 2017, Accepted 15 Jul 2018, Published online: 14 Aug 2018

References

  • A.S.T.M. Standard E8. 2004. Standard Test Method for Tension Testing of Metallic Materials. West Conshohocken (USA): ASTM, International.
  • Aigbodion, V. S., and S. B. Hassan. 2007. “Effect of Silicon Carbide Reinforcement on Microstructure and Properties of Cast Al-Si-Fe/SiC Particulate Composites.” Material Science and Engineering A 447: 355–360. doi:10.1016/j.msea.2006.11.030.
  • Akhlaghi, F., and Z. A. Bidaki. 2009. “Influence of Graphite Content on Dry Sliding and Oil Impregnated Sliding Wear Behaviour of Al2024-Gr Composite Produced by in Situ Powder Metallurgy Method.” Wear 266: 37–45. doi:10.1016/j.wear.2008.05.013.
  • Alidokht, S. A., Z. A. Abdollah, S. Soleymani, and H. Assadi. 2011. “Microstructure and Tribological Performance of an Aluminium Based Hybrid Composite Produced by Friction Stir Processing.” Material and Design 32: 2727–2733. doi:10.1016/j.matdes.2011.01.021.
  • Altinkok, N., and R. Koker. 2006. “Modelling of the Tensile and Density Properties in Particle Reinforced Metal Matrix Composites by Using Neural Networks.” Material and Design 27: 625–631. doi:10.1016/j.matdes.2005.01.005.
  • Baradeswaran, A., and A. E. Perumal. 2014. “Wear and Mechanical Characteristics of Al 7075/Graphite Composites.” Composites: Part B 56: 472–476. doi:10.1016/j.compositesb.2013.08.073.
  • Basavarajappa, S., G. Chandramohan, M. Arjun, T. Mukundan, R. Subramanian, and P. Gopalakrishnan. 2007. “Influence of Sliding Speed on the Dry Sliding Wear Behaviour and the Subsurface Deformation on Hybrid Metal Matrix Composite.” Wear 262: 1007–1012. doi:10.1016/j.wear.2006.10.016.
  • Feng, Y. C., L. Geng, P. Q. Zheng, Z. Z. Zheng, and G. S. Wang. 2008. “Fabrication and Characteristic of Al-Based Hybrid Composite Reinforced with Tungsten Oxide Particle and Aluminum Borate Whisker by Squeeze Casting.” Material and Design 29: 2023–2026. doi:10.1016/j.matdes.2008.04.006.
  • Hashim, J., L. Looney, and M. S. J. Hashmi. 1999. ““Metal Matrix Composites.” Journal of Material Processing Technology 92–93: 1–7. doi:10.1016/S0924-0136(99)00118-1.
  • Hassan, A. M., G. M. Tashtoush, and A. K. J. Ahmed. 2007. “Effect of Graphite And/Or Silicon Carbide Particles Addition on the Hardness and Surface Roughness of Al-4 Wt. % Mg Alloy.” Journal of Composite Material 41: 453–465. doi:10.1177/0021998306063804.
  • Hsu, C. J., C. Y. Chang, and P. W. Kao. 2006. “Al-Al3Ti Nanocomposites Produced in Situ by Friction Stir Processing.” ActaMaterialia 54: 5241–5249. doi:10.1016/j.actamat.2006.06.054.
  • Hu, C. M., C. M. Lai, and P. W. Kao. 2009. “Solute-Enhanced Tensile Ductility of Ultrafine-Grained Al-Zn Alloy Fabricated by Friction Stir Processing.” ScriptaMaterialia 60: 639–642. doi:10.1016/j.scriptamat.2008.12.031.
  • Kaczmar, J. W., K. Pietrzak, and W. Wlosinski. 2000. “The Production and Application of Metal Matrix Composite Materials.” Journal of Material Processing and Technology 106: 58–67. doi:10.1016/S0924-0136(00)00639-7.
  • Kerti, I., and F. Toptan. 2008. “Microstructural Variations in Cast B4C-reinforced Aluminium Matrix Composites (Amcs).” Material Letters 62: 1215–1218. doi:10.1016/j.matlet.2007.08.015.
  • Kok, M. 2005. “Production and Mechanical Properties of Al2O3 Particle-Reinforced 2024 Aluminium Alloy Composites.” Journal of Material Processing Technology 161: 381–387. doi:10.1016/j.jmatprotec.2004.07.068.
  • Kumar, G. B. V., C. S. P. Rao, and N. Selvaraj. 2012. “Studies on Mechanical and Dry Sliding Wear of Al6061-SiC Composites.” Composite Part B 43: 1185–1191. doi:10.1016/j.compositesb.2011.08.046.
  • Lashgari, H. R., A. R. Sufizadeh, and M. Emamy. 2010. “The Effect of Strontium on the Microstructure and Wear Properties of A356–10% B4C Cast Composites.” Material and Design 31: 2187–2195. doi:10.1016/j.matdes.2009.10.049.
  • Mortensen, A. 1988. Mechanical and Physical Behaviour of Metals and Ceramic Compounds, 141. Roskilde, Denmark: Riso National Laboratory.
  • Pai, B. C., K. G. Satyanarayana, and P. S. Robi. 1992. “Effect of Chemical and Ultrasound Treatment on the Tensile Properties of Carbon Fibers.” Material Science Letters 11: 779–781. doi:10.1007/BF00729491.
  • Prashant, S. N., N. Madeva, and V. Auradi. 2012. “Prepration and Evaluation of Mechanical and Wear Properties of 6061 Al Reinforced with Graphite Particulate Metal Matrix Composite.” International Journal of Metallurgical and Materials Science and Engineering 2 (3): 85–95.
  • Ramesh, C. S., R. Keshavamurthy, B. H. Channabasappa, and A. Abrar. 2009. “Microstructure and Mechanical Properties of Ni–P Coated Si3N4 Reinforced Al6061 Composites.” Material Science and Engineering A 502: 99–106. doi:10.1016/j.msea.2008.10.012.
  • Ravi, K. R., V. M. Sreekumar, R. M. Pillai, M. Chandan, K. R. Amaranathan, and K. R. Arul. 2007. “Optimization of Mixing Parameters through a Water Model for Metal Matrix Composites Synthesis.” Material and Design 28: 871–881. doi:10.1016/j.matdes.2005.10.007.
  • Rhodes, C. G., M. W. Mahoney, and W. H. Bingel. 2003. “Fine-Grain Evolution in Friction Stir Processed 7050 Aluminium.” ScriptaMaterialia 48: 1451–1455. doi:10.1016/S1359-6462(03)00082-4.
  • Riahi, A. R., and A. T. Alpas. 2001. “The Role of Tribo-Layers on the Sliding Wears Behavior of Graphitic Aluminum Matrix Composites.” Wear 251: 1396–1407. doi:10.1016/S0043-1648(01)00796-7.
  • Rohatgi, P. K., R. Guo, J. K. Kim, S. Rao, T. Stephenson, and T. Waner. 1997. Wear and Friction of Cast Aluminum–SiC–Gr Composites: Materials Solutions, on Wear of Engineering Materials Proceedings, 205–211. Indianapolis, Indiana.
  • Rohatgi, P. K., Y. Liu, and S. Ray. 2004. “Friction and Wear of Metal-Matrix Composites.” ASM Handbook 18: 801–811.
  • Sahin, Y. 2003. “Prepration and Some Properties of SiC Particle Reinforced Aluminium Alloy Composites.” Material and Design 24: 671–679. doi:10.1016/S0261-3069(03)00156-0.
  • Sahin, Y., and M. Acilar. 2003. “Production and Properties of SiCp Reinforced Aluminium Alloy Composites.” Composite Part A 34: 709–718. doi:10.1016/S1359-835X(03)00142-8.
  • Sajjadi, S. A., H. R. Ezatpour, and H. Beygi. 2010. “Microstructure and Mechanical Properties of Al-Al2O3 Micro and Nano Composites Fabricated by Stir Casting.” In Proceeding of 14th National Conference on Material Science and Engineering, 325–332. Tehran, Iran.
  • Sevik, H., and K. S. Can. 2006. “Properties of Alumina Particulate Reinforced Aluminium Alloy Produced by Pressure Die Casting.” Material and Design 27: 676–683. doi:10.1016/j.matdes.2005.01.006.
  • Sharma, P., G. Chauhan, and N. Sharma. 2013. “Production Of AMC By Stir Casting: An Overview.” International Journal of Contemporary Practices 2 (1): 23–46.
  • Sharma, P., D. Khandja, and S. Sharma. 2014. “Tribological and Mechanical Behavior of Particulate Aluminium Matrix Composites.” Journal of Reinforced Plastic and Composites 33 (23): 2192–2202. doi:10.1177/0731684414556012.
  • Sharma, P., D. Khanduja, and S. Sharma. 2014. “Metallurgical and Mechanical Characterization of Al6082-B4C/Si3N4 Hybrid Composites Manufactured by Combined Ball Milling and Stir Casting.” Applied Mechanics and Materials 592594: 484–488. doi:10.4028/www.scientific.net/AMM.592-594.484.
  • Sharma, P., D. Khanduja, and S. Sharma. 2015a. “Parametric Study of Dry Sliding Wear of Aluminium Metal Matrix Composites by Response Surface Methodology.” Material Today Proceedings 2 (45): 2687–2697. doi:10.1016/j.matpr.2015.07.234.
  • Sharma, P., D. Khanduja, and S. Sharma. 2015b. “Production of Hybrid Composite by a Novel Process and Its Physical Comparison with Single Reinforced Composites.” Material Today Proceedings 2 (45): 2698–2707. doi:10.1016/j.matpr.2015.07.236.
  • Sharma, P., D. Khanduja, and S. Sharma. 2016. “Dry Sliding Wear Investigation of Al6082/Gr Metal Matrix Composites by Response Surface Methodology.” Journal of Material Research and Technology 5 (1): 29–36. doi:10.1016/j.jmrt.2015.05.001.
  • Sharma, P., S. Sharma, and D. Khanduja. 2015a. “On the Use of Ball Milling for the Production of Ceramic Powders.” Material and Manufacturing Process 30: 1370–1376. doi:10.1080/10426914.2015.1037904.
  • Sharma, P., S. Sharma, and D. Khanduja. 2015b. “A Study on Microstructure of Aluminium Matrix Composites.” Journal of Asian Ceramic Societies 3 (3): 240–244. doi:10.1016/j.jascer.2015.04.001.
  • Sharma, P., S. Sharma, and D. Khanduja. 2015a. “Production and Some Properties of Si3N4 Reinforced Aluminium Alloy Composites.” Journal of Asian Ceramic Societies 3 (3): 352–359. doi:10.1016/j.jascer.2015.07.002.
  • Sharma, P., S. Sharma, and D. Khanduja. 2016a. “Effect of Graphite Reinforcement on Physical and Mechanical Properties of Aluminium Metal Matrix Composites.” Particulate Science and Technology 34 (1): 1–6. doi:10.1080/02726351.2015.1031924.
  • Sharma, P., S. Sharma, and D. Khanduja. 2016b. “Production and Characterization of AA6082-(Si3N4 + Gr) Stir Cast Hybrid Composites.” Particulate Science and Technology 35 (2): 158–165. doi:10.1080/02726351.2016.1143066.
  • Shorowordi, K. M., T. Laoui, A. S. M. A. Haseeb, J. P. Celis, and L. Froyen. 2003. ““Microstructure and Interface Characteristics of B4C, SiC, and Al2O3 Reinforced Al Matrix Composites.” Journal of Material Processing Technology 142: 738–743. doi:10.1016/S0924-0136(03)00815-X.
  • Surappa, M. K. 1997. “Microstructure Evolution during Solidification of DRMMC: State of Art.” Journal of Material Processing Technology 63: 325–333. doi:10.1016/S0924-0136(96)02643-X.
  • Suresh, S., N. S. V. Moorthi, S. C. Vettivel, N. Selvakumar, and G. R. Jinu. 2014. “Effect of Graphite Addition on Mechanical Behavior of Al6061/TiB2 Hybrid Composite Using Acoustic Emission.” Materials Science and Engineering A 612: 16–27. doi:10.1016/j.msea.2014.06.024.
  • Suresha, S., and B. K. Sridhara. 2010. “Effect of Silicon Carbide Particulates on Wear Resistance of Graphitic Aluminium Matrix Composites.” Material and Design 31: 4470–4477. doi:10.1016/j.matdes.2010.04.053.
  • Wang, W., Q. Y. Shi, and P. Liu. 2009. “A Novel Way to Produce Bulk SiC Reinforced Aluminium Metal Matrix Composites by Friction Stir Processing.” Journal of Material Processing Technology 209: 2099–2103. doi:10.1016/j.jmatprotec.2008.05.001.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.