On the toughness of thermoplastic polymer nanocomposites as assessed by the essential work of fracture (EWF) approach

, , , &
Pages 395-404 | Received 27 Feb 2013, Accepted 25 Apr 2013, Published online: 19 Jun 2013

References

  • Bárány , T , Czigány , T and Karger-Kocsis , J . 2010 . Application of the essential work of fracture (EWF) concept for polymers, related blends and composites . Progr. Polym. Sci. , 35 : 1257 – 1287 .
  • Martinez , AB , Gamez-Perez , J , Sanchez-Soto , M , Velasco , JI and Santana , OO . 2009 . Maspoch MLl. The essential work of fracture (EWF) method – analyzing the post-yielding fracture mechanics of polymers . Eng. Fract. Mech. , 16 : 2604 – 2617 .
  • Karger-Kocsis J. Chapter 12: On the toughness of “nanomodified” polymers and their traditional polymer composites. In: Karger-Kocsis J, Fakirov S, editors. Nano- and micromechanics of polymer blends and composites. Munich: Hanser; 2009. p. 426–470.
  • Utracki , LA . 2004 . Clay-containing polymeric nanocomposites , Shawbury : Rapra Technology .
  • Streller , RC , Thomann , R , Torno , O and Mülhaupt , R . 2009 . Morphology, crystallization behavior, and mechanical properties of isotactic poly(propylene) nanocomposites based on organophilic boehmite . Macromol. Mater. Eng. , 294 : 380 – 388 .
  • Ogunniran , ES , Sadiku , R , Sinha Ray , S and Luruli , Ny . 2012 . Morphology and thermal properties of compatibilized PA12/PP blends with boehmite alumina nanofillers inclusions . Macromol. Mater. Eng. , 297 : 627 – 638 .
  • Pedrazzoli D, Ceccato R, Karger-Kocsis J, Pegoretti A. Viscoelastic behaviour and fracture toughness of linear-low-density polyethylene reinforced with synthetic boehmite alumina nanoparticles. Express Polym. Lett. 2013;7:652–666.
  • Maspoch , MLl , Gámez-Perez , J , Gordillo , A , Sánchez-Soto , M and Velasco , JI . 2002 . Characterization of injected EPBC plaques using the essential work of fracture (EWF) method . Polymer. , 43 : 4177 – 4183 .
  • Karger-Kocsis , J . 1996 . For what kind of polymer is the toughness assessment by the essential work concept straightforward? . Polym. Bull. , 37 : 119 – 126 .
  • Karger-Kocsis , J and Bárány , T . 2002 . Plane-stress fracture behavior of syndiotactic polypropylenes of various crystallinity as assessed by the essential work of fracture method . Polym. Eng. Sci. , 42 : 1410 – 1419 .
  • Tuba T, Khumalo VM, Karger-Kocsis J. Essential work of fracture of poly(ϵ-caprolactone)/boehmite aluminananocomposites: effect of surface coating. J. Appl. Polym. Sci. 2013;129:2950–2958. doi:10.1002/app.39004
  • Michler , GH and Baltá-Calleja , FJ . 2012 . Nano- and micromechanics of polymers , Munich : Hanser .

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.