Joining of SiC ceramic by using the liquid polyvinylphenylsiloxane

, &
Pages 212-216 | Received 02 Aug 2017, Accepted 09 Oct 2017, Published online: 25 Oct 2017

References

  • Wang H, Zhou X, Yu J, et al. Fabrication of SiCf/SiC composites by chemical vapor infiltration and vapor silicon infiltration. Mater Lett. 2010;64:1691–1693. doi: 10.1016/j.matlet.2010.05.013
  • Colombo P, Sglavo V, Pippel E, et al. Joining of reaction-bonded silicon carbide using a preceramic polymer. J Mater Sci. 1998;33:2405–2412. doi: 10.1023/A:1004312109836
  • Lewinsohn C, Singh M, Shibayama T, et al. Joining of silicon carbide composites for fusion energy applications. J Nucl Mater. 2000;283–287:1258–1261. doi: 10.1016/S0022-3115(00)00247-6
  • Zhao S, Zhou X, Yu H, et al. Compatibility of PIP SiCf/SiC with LiPb at 700°C. Fusion Eng Des. 2010;85:1624–1626. doi: 10.1016/j.fusengdes.2010.04.060
  • Wang Z, Huang J, Zhang H, et al. Reactive composite brazing of Cf/SiC composites to Ti alloy with (Ag-6Al)+Ti + C composite filler materials. Mater Sci Technol. 2011;27:49–52. doi: 10.1179/174328409X418955
  • Lin G, Huang J, Zhang H, et al. Microstructure and mechanical performance of brazed joints of Cf/SiC composite and Ti alloy using Ag–Cu–Ti–W. Sci Technol Weld Join. 2006;11:379–383. doi: 10.1179/174329306X113235
  • Riccardi B, Nannetti C, Petrisor T, et al. Issues of low activation brazing of SiCf/SiC composites by using alloys without free silicon. J Nucl Mater. 2004;329–333:562–566. doi: 10.1016/j.jnucmat.2004.04.118
  • Halbig M, Singh M, Shpargel T, et al. Diffusion bonding of silicon carbide ceramics using titanium interlayers. Ceram Eng Sci Proc. 2006;27:133–143. doi: 10.1002/9780470291313.ch13
  • Jung Y-I, Kim SH, Kim HG, et al. Microstructures of diffusion bonded SiC ceramics using Ti and Mo interlayers. J Nucl Mater. 2013;441:510–513. doi: 10.1016/j.jnucmat.2013.07.008
  • Khachatryan G, Arutyunyan A, Kharatyan S. Activated combustion of a silicon–carbon mixture in nitrogen and SHS of Si3N4-SiC composite ceramic powders and silicon carbide. Combust Explos Shock Waves. 2006;42:543–548. doi: 10.1007/s10573-006-0086-7
  • Masanta M, Ganesh P, Kaul R, et al. Microstructure and mechanical properties of TiB2-TiC-Al2O3-SiC composite coatings developed by combined SHS, sol-gel and laser technology. Surf Coat Technol. 2010;204:3471–3480. doi: 10.1016/j.surfcoat.2010.04.018
  • Xu HB, Zhou BF, Luo QX, et al. The microstructure and properties of joint interface of semisolid stirring brazing of composites. J Mater Sci Technol. 2012;28:1163–1168. doi: 10.1016/S1005-0302(12)60187-X
  • Chen XG, Xie RS, Lai ZW, et al. Interfacial structure and formation mechanism of ultrasonic-assisted brazed joint of SiC ceramics with Al-12Si filler metals in air. J Mater Sci Technol. 2017;33:492–498. doi: 10.1016/j.jmst.2016.03.016
  • Yajima S, Hayashi J, Omori M, et al. Development of a silicon carbide fibre with high tensile strength. Nature. 1976;261:683–685. doi: 10.1038/261683a0
  • Katoh Y, Snead LL, Cheng T, et al. Radiation-tolerant joining technologies for silicon carbide ceramics and composites. J Nucl Mater. 2014;448(1):497–511. doi: 10.1016/j.jnucmat.2013.10.002
  • Liao NB, Xue W, Zhou HM, et al. Molecular dynamics investigation of structure and high-temperature mechanical properties of SiBCO ceramics. J Alloy Compd. 2014;610:45–49. doi: 10.1016/j.jallcom.2014.04.189
  • Greil P. Active-filler-controlled pyrolysis of preceramic polymers. J Am Ceram Soc. 1995;78(4):835–848. doi: 10.1111/j.1151-2916.1995.tb08404.x
  • Wang XZ, Wang J, Wang H. Synthesis of a novel preceramic polymer (V-PMS) and its performance in heat-resistant organic adhesives for joining SiC ceramic. J Eur Ceram Soc. 2012;32:3415–3422. doi: 10.1016/j.jeurceramsoc.2012.03.032
  • Fang Y, Huang M, Yu Z, et al. Synthesis, characterization, and pyrolytic conversion of a novel liquid polycarbosilane. J Am Ceram Soc. 2008;91:3298–3302. doi: 10.1111/j.1551-2916.2008.02603.x
  • Liu HL, Li SJ, Chen ZJ. Joining of reaction-bonded silicon carbide using a polysiloxane. Rare Metal Mater Eng. 2006;35(1):134–135.
  • Xiong HP, Chen B, Kang YS, et al. Wettability of Co-V, and PdNi-Cr-V system alloys on SiC ceramic and interfacial reactions. Scr Mater. 2007;56:173–176. doi: 10.1016/j.scriptamat.2006.08.067
  • Wei Q, Pippel E, Woltersdorf J, et al. Interfacial SiC formation in polysiloxane-derived Si-O-C ceramics. Mater Chem Phys. 2002;73:281–289. doi: 10.1016/S0254-0584(01)00395-9
  • Wang C, Wang J, Park CB, et al. Cross-linking behavior of a polysiloxane in preceramic foam processing. J Mater Sci. 2004;39:4913–4915. doi: 10.1023/B:JMSC.0000035335.92101.7c
  • Renlund GM, Prochazka S, Doremus RH. Silicon oxycarbide glasses: part II. Structures and properties. J Mater Res. 1991;6(12):2723–2734. doi: 10.1557/JMR.1991.2723
  • Lefebvre J, Mamleev V, Le Bras M, et al. Kinetic analysis of pyrolysis of cross-linked polymers. Polym Degrad Stabil. 2005;88:85–91. doi: 10.1016/j.polymdegradstab.2004.02.020

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.