Effect of sintering temperature on the microstructures and mechanical properties of sodalite infiltrate all-ceramic material for dental restorations

, ORCID Icon, ORCID Icon & ORCID Icon
Pages 291-302 | Received 29 Jun 2017, Accepted 09 Nov 2017, Published online: 24 Nov 2017

References

  • Gu Y, Liu X, Meng G, et al. Porous YSZ ceramics by water-based gelcasting. Ceram Int. 1999;25(8):705–709. doi: 10.1016/S0272-8842(99)00005-X
  • Liu R, Wang CA. Synthesis of aluminum-doped mesoporous zirconia with improved thermal stability. Micropor Mesopor Mater. 2014;186:1–6. doi: 10.1016/j.micromeso.2013.11.024
  • Gain AK, Song HY, Lee BT. Microstructure and mechanical properties of porous yttria stabilized zirconia ceramic using poly methyl methacrylate powder. Scr Mater. 2006;54(12):2081–2085. doi: 10.1016/j.scriptamat.2006.03.009
  • Saremi M, Afrasiabi A, Kobayashi A. Microstructural analysis of YSZ and YSZ/Al2O3 plasma sprayed thermal barrier coatings after high temperature oxidation. Surf Coat Technol. 2008;202(14):3233–3238. doi: 10.1016/j.surfcoat.2007.11.029
  • Hu L, Wang CA, Huang Y. Porous yttria-stabilized zirconia ceramics with ultra-low thermal conductivity. J Mater Sci. 2010;45(12):3242–3246. doi: 10.1007/s10853-010-4331-9
  • Chen F, Cao F, Pan H, et al. Mechanical and dielectric properties of silicon nitride ceramics with high and hierarchical porosity. Mater Des. 2012;40:562–566. doi: 10.1016/j.matdes.2012.03.026
  • Ohji T, Fukushima M. Macro-porous ceramics: processing and properties. Int Mater Rev. 2012;57(2):115–131. doi: 10.1179/1743280411Y.0000000006
  • Feng Y, Wang K, Yao J, et al. Effect of the addition of polyvinylpyrrolidone as a pore-former on microstructure and mechanical strength of porous alumina ceramics. Ceram Int. 2013;39(7):7551–7556. doi: 10.1016/j.ceramint.2013.03.007
  • Liu R, Li Y, Wang CA, et al. Fabrication of porous alumina–zirconia ceramics by gel-casting and infiltration methods. Mater Des. 2014;63:1–5. doi: 10.1016/j.matdes.2014.05.061
  • Ohji T. Porous ceramic materials. In: Somiyas S, editor. Hand book of advanced ceramics. 2nd ed. Waltham, MA: Elsevier Inc.; 2013. p. 1131–1148.
  • Marple BR, Green DJ. Graded compositions and microstructures by infiltration processing. J Mater Sci. 1993;28(17):4637–4643. doi: 10.1007/BF00414252
  • Tu WC, Lange FF. Liquid precursor infiltration processing of powder compacts: I, kinetic studies and microstructure development. J Am Ceram Soc. 1995;78(12):3277–3282. doi: 10.1111/j.1151-2916.1995.tb07965.x
  • Lin YJ, Chen YC. Cyclic infiltration of porous zirconia preforms with a liquid solution of mullite precursor. J Am Ceram Soc. 2001;84(1):71–78. doi: 10.1111/j.1151-2916.2001.tb00610.x
  • Claus H. Vita In-Ceram, a new system for producing aluminum oxide crown and bridge substructures. Quintessence Dent Technol. 1990;16:35–46.
  • Hornberger H, Marquis PM. Mechanical properties and microstructure of In-Ceram, a ceramic-glass composite for dental crowns. Glass Sci Technol. 1995;68(6):188–194.
  • McLaren EA, White SN. Glass-infiltrated zirconia/alumina-based ceramic for crowns and fixed partial dentures. Pract Periodontics Aesthet Dent. 1999;11(8):985–994.
  • Guazzato M, Albakry M, Quach L, et al. Influence of surface and heat treatments on the flexural strength of a glass-infiltrated alumina/zirconia-reinforced dental ceramic. Dent Mater. 2005;21(5):454–463. doi: 10.1016/j.dental.2004.07.010
  • Guazzato M, Albakry M, Ringer SP, et al. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics. Dent Mater. 2004;20(5):449–456. doi: 10.1016/j.dental.2003.05.002
  • Chevalier J, Cales B, Drouin JM. Low-temperature aging of Y-TZP ceramics. J Am Ceram Soc. 1999;82(8):2150–2154. doi: 10.1111/j.1151-2916.1999.tb02055.x
  • Guess PC, Kuliš A, Witkowski S, et al. Shear bond strengths between different zirconia cores and veneering ceramics and their susceptibility to thermocycling. Dent Mater. 2008;24(11):1556–1567. doi: 10.1016/j.dental.2008.03.028
  • Borchers L, Stiesch M, Bach FW, et al. Influence of hydrothermal and mechanical conditions on the strength of zirconia. Acta Biomater 2010;6(12):4547–4552. doi: 10.1016/j.actbio.2010.07.025
  • Yao J, Wang H, Ratinac KR, et al. Formation of colloidal hydroxy-sodalite nanocrystals by the direct transformation of silicalite nanocrystals. Chem Mater. 2006;18(6):1394–1396. doi: 10.1021/cm052731+
  • Meier WM, Olson DH, Baerlocher C. Atlas of zeolite structure types. 4th ed. Amsterdam: Elsevier; 1996.
  • Baerlocher C, McCusker LB, Olsen DH. Atlas of zeolite framework types. 6th ed. Amsterdam: Elsevier; 2007.
  • Ocanto F, Álvarez R, de Navarro CU, et al. Influence of the alkalinity and NO3−/Cl− anionic composition on the synthesis of the cancrinite–sodalite system. Micropor Mesopor Mater. 2008;116(1):318–322. doi: 10.1016/j.micromeso.2008.04.019
  • Evsyunin VG, Sapozhnikov AN, Rastsvetaeva RK, et al. Crystal structure of the potassium-rich hauyne from Arissia (Italy). Crystallogr Rep. 1996;41(4):622–625.
  • Khajavi S, Sartipi S, Gascon J, et al. Thermostability of hydroxy sodalite in view of membrane applications. Micropor Mesopor Mater. 2010;132(3):510–517. doi: 10.1016/j.micromeso.2010.03.035
  • Cruciani G. Zeolites upon heating: factors governing their thermal stability and structural changes. J Phys Chem Solids. 2006;67(9):1973–1994. doi: 10.1016/j.jpcs.2006.05.057
  • Alberti A, Martucci A. Reconstructive phase transitions in microporous materials: rules and factors affecting them. Micropor Mesopor Mater. 2011;141(1):192–198. doi: 10.1016/j.micromeso.2010.11.014
  • Alberti A, Martucci A. Phase transformations and structural modifications induced by heating in microporous materials. Stud Surf Sci Catal. 2005;155:19–43. doi: 10.1016/S0167-2991(05)80135-1
  • Khajavi S, Kapteijn F, Jansen JC. Synthesis of thin defect-free hydroxy sodalite membranes: New candidate for activated water permeation. J Membr Sci. 2007;299(1):63–72. doi: 10.1016/j.memsci.2007.04.027
  • Sharp ZD, Helffrich GR, Bohlen SR, et al. The stability of sodalite in the system NaAlSiO4-NaCl. Geochim Cosmochim Acta. 1989;53(8):1943–1954. doi: 10.1016/0016-7037(89)90315-3
  • Wellman TR. The vapor pleasure of NaCl over decomposing sodalite. Geochim Cosmochim Acta. 1969;33(10):1302–1303. doi: 10.1016/0016-7037(69)90048-9
  • VITA In-Ceram, VITA Zahnfabrik. Directions for use, Vita Zahnfabrik Publication #187E–1190 Bad Sackinge. Germany; 2007.
  • I.O.f.S. (ISO) ISO 6872. Dentistry – Ceramic Materials; 2015.
  • Naji GA, Omar RA, Yahya R, et al. Sodalite zeolite as an alternative all-ceramic infiltrating material for alumina and zirconia toughened alumina frameworks. Ceram Int. 2016;42(10):12253–12261. doi: 10.1016/j.ceramint.2016.04.171
  • Naji GA, Omar RA, Yahya R. The effect of sodalite zeolite infiltrated material on the fracture toughness, elastic modulus and optical properties of all-ceramic dental prostheses. Ceram Int. 2016;42(16):18737–18746. doi: 10.1016/j.ceramint.2016.09.013
  • Naji GA, Omar RA, Yahya R. Influence of sodalite zeolite infiltration on the coefficient of thermal expansion and bond strength of all-ceramic dental prostheses. J Mech Behav Biomed Mater. 2017;67:135–143. doi: 10.1016/j.jmbbm.2016.12.007
  • Kwok K, Kiesel L, Frandsen HL, et al. Strength characterization of tubular ceramic materials by flexure of semi-cylindrical specimens. J Eur Ceram Soc. 2014;34(5):1423–1432. doi: 10.1016/j.jeurceramsoc.2013.12.005
  • Guazzato M, Albakry M, Swain MV, et al. Mechanical properties of in-ceram alumina and in-ceram zirconia. Int J Prosthodont. 2002;15(4):339–346.
  • Al-Makramani BMA. Clinical and mechanical evaluation of a new all-ceramic restorative material turkom-cera. Thesis submitted in fulfillment of the requirements for the degree of doctor of philosophy. University of Malaya, Kuala Lumpur; 2010.
  • Nabavi MS, Mohammadi T, Kazemimoghadam M. Hydrothermal synthesis of hydroxy sodalite zeolite membrane: separation of H2/CH4. Ceram Int. 2014;40(4):5889–5896. doi: 10.1016/j.ceramint.2013.11.033
  • Julbe A, Motuzas J, Cazevielle F, et al. Synthesis of sodalite/αAl2O3 composite membranes by microwave heating. Sep Purif Technol. 2003;32(1):139–149. doi: 10.1016/S1383-5866(03)00027-3
  • Pulgarin HL, Albano MP. Three different alumina–zirconia composites: sintering, microstructure and mechanical properties. Mater Sci Eng A. 2015;639:136–144. doi: 10.1016/j.msea.2015.05.010
  • Naga SM, Hassan AM, El-Maghraby HF, et al. In-situ sintering reaction of Al2O3–LaAl11O18–ZrO2 composite. Int J Refract Metals Hard Mater. 2016;54:230–236. doi: 10.1016/j.ijrmhm.2015.07.026
  • Chandrasekhar S, Pramada PN. Thermal studies of low silica zeolites and their magnesium exchanged forms. Ceram Int. 2002;28(2):177–186. doi: 10.1016/S0272-8842(01)00075-X
  • Clarke DR. Interpenetrating phase composites. J Am Ceram Soc. 1992;75(4):739–758. doi: 10.1111/j.1151-2916.1992.tb04138.x
  • Giordano RA, Pelletier L, Campbell S, et al. Flexural strength of an infused ceramic. glass ceramic, and feldspathic porcelain. J Prosthet Dent. 1995;73(5):411–418. doi: 10.1016/S0022-3913(05)80067-8
  • Ma JF, Wang SQ, Du RX, et al. Pressureless sintering of gel cast ZTA-MgO-TiO2 systems as potential dental ceramics. Adv Appl Ceram. 2011;110:275–279. doi: 10.1179/1743676111Y.0000000010
  • Mollazadeh S, Javadpour J, Eftekhari Yekta B, et al. Synthesis and characterisation of dental composite materials reinforced with fluoroapatite-mullite glass-ceramic particles. Adv Appl Ceram. 2013;112:294–300. doi: 10.1179/1743676112Y.0000000075
  • Anusavice KJ, Kakar K, Ferree N. Which mechanical and physical testing methods are relevant for predicting the clinical performance of ceramic-based dental prostheses? Clin Oral Implants Res. 2007;18(s3):218–231. doi: 10.1111/j.1600-0501.2007.01460.x
  • Ban S, Anusavice KJ. Influence of test method on failure stress of brittle dental materials. J Dent Res. 1990;69(12):1791–1799. doi: 10.1177/00220345900690120201
  • Kelly JR. Perspectives on strength. Dent Mater. 1995;11(2):103–110. doi: 10.1016/0109-5641(95)80043-3

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.