Publication Cover
Advances in Applied Ceramics
Structural, Functional and Bioceramics
Volume 117, 2018 - Issue 4
124
Views
0
CrossRef citations to date
0
Altmetric
Original Articles

Effects of thermal oxidising exposure on the tensile strength of Hi-Nicalon fibres

&
Pages 243-247 | Received 29 May 2017, Accepted 20 Aug 2017, Published online: 15 Feb 2018

References

  • Swain J, Gaurav K, Singh D, et al. A brief review on ceramic matrix composites, it’s attributes and it’s utility in future generation gas turbine. Inter J Innov Res in Sci Technol. 2014;1:290–292.
  • Naslain: R. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview. Compos Sci Technol. 2004;64:155–157. doi: 10.1016/S0266-3538(03)00230-6
  • Katoh Y, Snead LL, Henager JCH, et al. Current status and recent research achievements in SiC/SiC composites. J Nucl Mater. 2014;455:387–397. doi: 10.1016/j.jnucmat.2014.06.003
  • Lamon J, R’Mili M. Resistance to fatigue at intermediate temperatures in air for SiC Hi-Nicalon fibers: statistical distributions of lifetimes and strength degradation. J Am Ceram Soc. 2012;95:3613–3621. doi: 10.1111/j.1551-2916.2012.05414.x
  • Morishita K, Matsumoto T, Ochiai S, et al. Degradation mechanism of amorphous silicon carbide fiber due to air-exposure at high temperatures. Mater Trans. 2007;48:111–116. doi: 10.2320/matertrans.48.111
  • Takeda M, Urano A, Sakamoto J, et al. Microstructure and oxidative degradation behavior of silicon carbide fiber Hi-Nicalon type S. J Nucl Mater. 1998;258-263:1594–1599. doi: 10.1016/S0022-3115(98)00223-2
  • Xu WB, Zok FW, McMeeking RM. Model of oxidation-induced fiber fracture in SiC/SiC composites. J Am Ceram Soc. 2014;97:3676–3683. doi: 10.1111/jace.13180
  • Wu SJ, Cheng LF, Zhang LT. Oxidation behavior of 3D Hi-Nicalon/SiC composite exposed in wet and simulated air environments. Corros Sci. 2013;66:111–117. doi: 10.1016/j.corsci.2012.09.008
  • Martínez-Fernández J, Morscher GN. Room and elevated temperature tensile properties of single tow Hi-Nicalon, carbon interphase, CVI SiC matrix minicomposites. J Eur Ceram Soc 2000;20:2627–2636. doi: 10.1016/S0955-2219(00)00138-2
  • Wu SJ, Cheng LF, Zhang Q, et al. Thermophysical and mechanical properties of a three-dimensional Hi-Nicalon/SiC composite. Int J App Ceram Tchnol. 2006;3:75–79. doi: 10.1111/j.1744-7402.2006.02056.x
  • Takeda M, Sakamoto J, Imai Y, et al. Thermal stability of the low-oxygen-content silicon carbide fiber, Hi-NicalonTM. Compos Sci Technol. 1999;59:813–819. doi: 10.1016/S0266-3538(99)00012-3
  • Chu MC, Cho SJ, Lee YC, et al. Crack healing in silicon carbide. J Am Ceram Soc. 2004;87:490–492. doi: 10.1111/j.1551-2916.2004.00490.x
  • Gou YZ, Wang H, Jian K. Formation of carbon-rich layer on the surface of SiC fiber by sintering under vacuum for superior mechanical and thermal properties. J Eur Ceram Soc. 2017;37:907–914. doi: 10.1016/j.jeurceramsoc.2016.10.013
  • Nan CW, Li XP, Cai KF, et al. Grain size-dependent elastic moduli of nanocrystals. J Mater Sci Lett. 1998;17:1917–1919. doi: 10.1023/A:1006652224897
  • García Ferré F, Mairov A, Ceseracciu L, Serruys Y, et al. Radiation endurance in Al2O3 nanoceramics. Sci Rep 2016;6:33478. doi: 10.1038/srep33478
  • Knudsen FP. Dependence of mechanical strength of brittle polycrystalline specimens on porosity and grain size. J Am Ceram Soc. 1959;42:376–387. doi:10.1111/j.1151-2916.1959.tb13596.x.
  • Youngblood GE, Lewinsohn CA, Jones RH, et al. Tensile strength and fracture surface characterization of Hi-NicalonTM SiC fibers. J Nucl Mater 2001;289:1–9. doi: 10.1016/S0022-3115(00)00675-9
  • Miyoshi H, Yamada K, Kohmura K, et al. Theoretical investigation of dielectric constant and elastic modulus of three-dimensional isotropic porous silica film with cubic and disordered pore arrangements. Jpn J Appl Phys. 2005;44:5982–5986. doi: 10.1143/JJAP.44.5982
  • Shuman DJ, Costa ALM, Andrade MS. Calculating the elastic modulus from nanoindentation and microindentation reload curves. Mater Charact. 2007;58:380–389. doi: 10.1016/j.matchar.2006.06.005
  • Gaudio PD, Behrens H, Deubener J. Viscosity and glass transition temperature of hydrous float glass. J Non-Cryst Solids. 2007;353:223–236. doi: 10.1016/j.jnoncrysol.2006.11.009
  • Karki BB, Stixrude L. First-principles study of enhancement of transport properties of silica melt by water. Phys Rev Lett 2015;104:215901. doi: 10.1103/PhysRevLett.104.215901
  • Wu SJ, Cheng LF, Zhang J, et al. Tension-tension fatigue damage characteristics of a 3D SiC/SiC composite in H2O-O2-Ar environment at 1300°C. Mater Sci Eng A. 2006;435–436:412–417. doi: 10.1016/j.msea.2006.07.041

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.