References
- Barsoum MW. MAX phases: properties of machinable ternary carbides and nitrides, Wiley-VCH. Weinheim. 2013. doi:10.1002/9783527654581.
- Sun ZM. Progress in research and development on MAX phases: a family of layered ternary compounds. Int. Mater. Rev. 2011;56:143–166. doi:10.1179/1743280410Y.0000000001.
- Rangaraj L, Divakar C, Jayaram V. MAX phases and Ultra-high temperature ceramics for Extreme Environments. IGI Global. 2013. doi:10.4018/978-1-4666-4066-5.
- Haftani M, Saeedi Heydari M, Baharvandi HR, et al. Studying the oxidation of Ti2AlC MAX phase in atmosphere: a review. Int J Refract Met Hard Mater. 2016;61:51–60. doi:10.1016/j.ijrmhm.2016.07.006.
- Xiao QD, Lv ZL. Current carrying friction and wear characteristics of Ti3AlC2 by novel method of infiltration sintering. Adv. Appl. Ceram. 2012;111:202–207. doi:10.1179/1743676111Y.0000000066.
- Zhou W, Li K, Zhu J, et al. In situ synthesis, mechanical and cyclic oxidation properties of Ti3AlC2/Al2O3 composites. Adv. Appl. Ceram. 2018;117:340–346. doi:10.1080/17436753.2018.1434953.
- Fu H, Liu W, Gao TAO. Structural, elastic and thermodynamic properties of Ti2SC, Bull. Mater. Sci. 2011;34:1617–1625. doi:10.1007/s12034-011-0367-y.
- Cui S, Feng W, Hu H, et al. Hexagonal Ti2SC with high hardness and brittleness: a first-principles study. Scr. Mater. 2009;61:576–579. doi:10.1016/j.scriptamat.2009.05.026.
- Gupta S, Amini S, Filimonov D, et al. Tribological behavior of Ti2SC at ambient and elevated temperatures. J. Am. Ceram. Soc. 2007;90:3566–3571. doi:10.1111/j.1551-2916.2007.01950.x.
- Li X, Liang B, Li Z. Combustion synthesis of Ti2SC. Int. J. Mater. Res. 2013;104:1038–1040. doi:10.3139/146.110972.
- Guan C, Sun N. Synthesis of high-purity Ti2SC powder by microwave hybrid heating. J. Adv. Ceram. 2016;5:337–343. doi:10.1007/s40145-016-0207-z.
- Guan C, Sun N. Synthesis and tribological properties of high purity Ti2SC nanolamellas by microwave hybrid heating. J. Alloys Compd. 2017;699:25–30. doi:10.1016/j.jallcom.2016.12.329.
- Guan CL. Rapid and low temperature synthesis of high purity Ti2SC powder by microwave hybrid heating. Adv. Appl. Ceram. 2016;115:470–472. doi:10.1179/1743676115Y.0000000032.
- Zhou W, Liu L, Zhu J, et al. Facile synthesis of high-purity Ti2SC powders by spark plasma sintering technique. Ceram. Int. 2017;43:9363–9368. doi:10.1016/j.ceramint.2017.04.104.
- Chen K, Ye Q, Zhou J, et al. Synthesis of Ti2SC phase using iron disulfide or iron sulfide post-treated with acid. J. Am. Ceram. Soc. 2015;98:1074–1079. doi:10.1111/jace.13457.
- Hoseini SM, Heidarpour A, Ghasemi S. On the mechanism of mechanochemical synthesis of Ti2SC from Ti/FeS2/C mixture. Adv. Powder Technol. 2019;30:1672–1677. doi:10.1016/j.apt.2019.05.017.
- Zarezadeh Mehrizi M, Beygi R, Eisaabadi BG, et al. Mechanically activated combustion synthesis of Ti3AlC2/Al2O3 nanocomposite from TiO2/Al/C powder mixtures. Adv. Powder Technol. 2018. doi:10.1016/j.apt.2018.11.007.
- Takacs L. Self-sustaining reactions induced by ball milling. Prog. Mater. Sci. 2002;47:355–414. doi: 10.1016/S0079-6425(01)00002-0
- Yang C, Jin SZ, Liang BY, et al. Synthesis of Ti3AlC2 ceramic by high-energy ball milling of elemental powders of Ti, Al and C. J. Mater. Process. Technol. 2009;209:871–875. doi:10.1016/j.jmatprotec.2008.02.056.
- Zhu JF, Qi GQ, Wang F, et al. Synthesis of Ti3AlC2/Al2O3 nanopowders by mechano-chemical reaction. Adv. Powder Technol. 2010;21:578–581. doi:10.1016/j.apt.2010.03.010.
- Shahin N, Kazemi S, Heidarpour A. Mechanochemical synthesis mechanism of Ti3AlC2 MAX phase from elemental powders of Ti, Al and C. Adv. Powder Technol. 2016;27:1775–1780. doi:10.1016/j.apt.2016.06.008.
- Hendaoui A, Vrel D, Amara A, et al. Synthesis of high-purity polycrystalline MAX phases in Ti–Al–C system through mechanically activated self-propagating high-temperature synthesis. J. Eur. Ceram. Soc. 2010;30:1049–1057. doi:10.1016/j.jeurceramsoc.2009.10.001.
- Turki F, Abderrazak H, Schoenstein F, et al. SPS parameters influence on Ti3SiC2 formation from Si/TiC: mechanical properties of the bulk materials. J. Alloys Compd. 2017;708:123–133. doi:10.1016/j.jallcom.2017.02.304.
- Feng L, Lee S, Lee H. Nano-sized zirconium carbide powder: synthesis and densification using a spark plasma sintering apparatus. Int J Refract Met Hard Mater. 2017;64:98–105. doi:10.1016/j.ijrmhm.2017.01.006.
- Bin Zhu W, Song JH, Mei BC. Kinetics and microstructure evolution of Ti2SC during in situ synthesis process. J. Alloys Compd. 2013;566:191–195. doi:10.1016/j.jallcom.2013.03.032.