XRD and XANES study of reactions in particulate Al–Mg alloy composites

, &
Pages 54-60 | Received 23 Jan 2010, Accepted 09 Aug 2010, Published online: 22 Nov 2013

References

  • Bouzoubaâ N, Fournier B: ‘Current situation with the production and use of supplementary cementitious materials (SCMs) in concrete construction in Canada’, Can. J. Civ. Eng., 2005, 32, 129–143.
  • Tishmack JK, Burns PE: ‘The chemistry and mineralogy of coal and coal combustion products’, Geol. Soc. Spec. Publ., 2004, 236, 223–246.
  • Adriano DC, Page AL, Elseewi AA, Chang AC, Straughan I: ‘Utilization and disposal of fly ash and other coal residues in terrestrial ecosystems: a review’, J. Environ. Qual., 1980, 9, (3), 333–344.
  • McBride SP, Shukla A, Bose A: ‘Processing and characterization of a lightweight concrete using cenospheres’, J. Mater. Sci., 2002, 37, (19), 4217–4225.
  • Rohatgi PK, Weiss D, Gupta N: ‘Applications of fly ash in synthesizing low‐cost MMCs for automotive and other applications’, JOM, 2006, 58, (11), 71–76.
  • Guo R, Venugopalan D, Rohatgi PK: ‘Differential thermal analysis to establish the stability of aluminum–fly ash composites during synthesis and reheating’, Mater. Sci. Eng. A, 1998, A241, (1–2), 184–190.
  • Wu GH, Dou ZY, Jiang LT, Cao JH: ‘Damping properties of aluminum matrix–fly ash composites’, Mater. Lett., 2006, 60, 2945–2948.
  • Rajan TPD, Pillai RM, Pai BC, Satyanarayana KG, Rohatgi PK: ‘Fabrication and characterization of Al–7Si–0.35Mg/fly ash metal matrix composites processed by different stir casting routes’, Compos. Sci. Technol., 2007, 67, 3369–3377.
  • Rohatgi PK, Gajdardziska‐Josifovska M, Robertson DP, Kim JK, Guo RQ: ‘Age‐hardening characteristics of aluminum alloy–hollow fly ash composites’, Metall. Mater. Trans. A, 2002, 33A, (5), 1541–1547.
  • Ramachandra M, Radhakrishna K: ‘Effect of reinforcement of fly ash on sliding wear, slurry erosive wear and corrosive behavior of aluminium matrix composite’, Wear, 2007, 262, (11–12), 1450–1462.
  • Ramachandra M, Radhakrishna K: ‘Synthesis‐microstructure‐mechanical properties‐wear and corrosion behavior of an Al–Si (12%)–flyash metal matrix composite’, J. Mater. Sci., 2005, 40, (22), 5989–5997.
  • Ramachandra M, Radhakrishna K: ‘Microstructure, mechanical properties, wear and corrosion behaviour of Al–Si/flyash composite’, Mater. Sci. Technol., 2005, 21, (11), 1337–1343.
  • He MY, Kiser M, Wu B, Zok FW: ‘Influence of thermal expansion mismatch on residual stresses and flow response of microballoon composites’, Mech. Mater., 1996, 23, (2), 133–146.
  • Escalera‐Lozano R, Gutiérrez CA, Pech‐Canul MA, Pech‐Canul MI: ‘Corrosion characteristics of hybrid Al/Sicp/MgAl2O4 composites fabricated with fly ash and recycled aluminum’, Mater. Charact., 2007, 58, (10), 953–960.
  • Sobczak N, Sobczak J, Morgiel J, Stobierski L: ‘TEM characterization of the reaction products in aluminium–fly ash couples’, Mater. Chem. Phy., 2003, 81, 296–300.
  • Pech‐Canul MI, Escalera‐Lozano R, Pech‐Canul MA, Rendón‐Angeles JC, López‐Cuevas J: ‘Degradation processes in Al/SiCp/MgAl2O4 composites prepared from recycled aluminum with fly ash and rice hull ash’, Mater. Corros., 2007, 58, (11), 833–840.
  • Winburn RS, Grier DG, McCarthy GJ, Peterson RB: ‘Rietveld quantitative X‐ray diffraction analysis of NIST fly ash standard reference materials’, Powder Diffr., 2000, 15, (3), 163–72.
  • McCarthy GJ: ‘X‐ray powder diffraction for studying the mineralogy of fly ash’, in ‘Fly ash and coal conversion by‐products: characterization, utilization and disposal’, (ed. , McCarthy G J, et al.), Vol. 113, 75–86; 1988, Pittsburgh, PA, Materials Research Society.
  • Glasser FP: ‘Coal combustion wastes: characterization, reuse and disposal’, Geol. Soc. Spec. Publ., 2004, 236, (1), 211–222.
  • Lawniczak‐Jablonska K, Iwanowski RJ, Demchenko IN, Boettcher T, Einfeldt S, Hommel D, Cortes R, Perera RCC: ‘Polarization dependent X‐ray absorption studies of the chemical bonds anisotropy in wurtzite GaN grown at different conditions’, J. Alloys Compos., 2001, 328, 77–83.
  • Piskorska E, Lawniczak‐Jablonska K, Minikayev R, Wolska A, Paszkowicz W, Klimczyk P, Benko E: ‘Quantitative phase analysis of cubic boron nitride based composites by X‐ray absorption near edge structure’, Spectrochim. Acta B, 2007, 62B, 461–469.
  • Piskorska E, Lawniczak‐Jablonsska K, Demchenko IN, Benko E, Welter E: ‘X‐ray absorption studies of phase formation in a Ti/TiN coating on cubic boron nitride’, J. Alloys Compos., 2004, 362, 171–177.
  • Lalvani SB, Croft M: ‘X‐ray absorption spectroscopy of amorphous alloys’, J. Mater. Sci Lett., 1999, 18, 1281–1283.
  • Mondal K, Sathitsuksanoh N, Croft M, Lalvani SB: ‘X‐ray absorption spectroscopic analysis of amorphous Cr–P obtained via electrodeposition’, J. Mater. Sci. Lett., 2003, 22, 655–657.
  • Gikunoo E: ‘Effect of fly ash particles on the mechanical properties and microstructure of aluminum casting alloy A535’, MSc thesis, Saskatoon, SK, Canada, University of Saskatchewan, 2005.
  • Zou Z, Hu Y‐F, Sham TK, Huang HH, Xu GQ, Seet CS, Chan L: ‘XAFS studies of Al/TiNx films on Si(100) at the Al K‐ and L3,2‐edge’, J. Synch. Rad., 1999, 6, 524–525.
  • Kasrai M, Lennard WN, Brunner RW, Bancroft GM, Bardwell JA, Tan KH: ‘Sampling depth of total electron and fluorescence measurements in Si L‐ and K‐edge absorption spectroscopy’, Appl. Surf. Sci., 1996, 99, (4), 303–312.
  • Jones RG, Woodruff DP: ‘Sampling depths in total yield and reflectivity SEXAFS studies in the soft X‐ray region’, Surf. Sci., 1982, 114, 38–46.
  • Hu YF: Private communication, Canadian Light Source, Saskatoon, SK, Canada, 2010.
  • Pereira G, Lachenwitzer A, Nicholls MA, Kasrai M, Norton PR, de Stasio G: ‘Chemical characterization and nanomechanical properties of antiwear films fabricated from ZDDP on a near hypereutectic Al–Si alloy’, Tribol. Lett., 2005, 18, (4), 411–427.
  • Ildefonse P, Calas G, Flank AM, Lagarde P: ‘Low Z elements (Mg, Al, and Si) K‐edge X‐ray absorption spectroscopy in minerals and disordered systems’, Nucl. Instrum. Methods Phys. Res. B, 1995, 97B, 172–175.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.