Initial corrosion attack of 304L and T22 in 2 MW biomass gasifier: a microstructural investigation

, , , &
Pages 197-204 | Received 16 Apr 2014, Accepted 02 Jul 2014, Published online: 19 Jan 2015

References

  • Higman C and Burgt M: ‘Gasification’, 2nd edn; 2008, Houston, TX, Gulf Publishing.
  • P. Basu: ‘Biomass gasification and pyrolysis: Practical design and theory; 2010, Academic Press.
  • Larsson A, Seemann M Neves D and Thunman H: ‘Evaluation of performance of industrial-scale dual fluidized bed gasifiers using the chalmers 2–4-MWth gasifier’, Energy Fuels, 2013, 27, (11), 6665–6680.
  • Jonsson T, Froitzheim J, Pettersson J, Svensson J.-E, Johansson L.-G and Halvarsson M: ‘The influence of KCl on the corrosion of an austenitic stainless steel (304L) in oxidizing humid conditions at 600°C: A microstructural study’, Oxid. Met., 2009, 72, (3), 213–239.
  • Rahmel A and Tobolsky J: Corros. Sci., 1965, 5, 333–346.
  • Galerie A, Wouters Y and Caillet M: ‘The kinetic behaviour of metals in water vapor at high temperature; Can general rules be proposed?’, Mater. Sci. Forum, 2001, 369–372, 231–238.
  • Ehlers J, Young DJ, Smaardijk EJ, Tyagi AK, Penkalla HJ, Singheiser L and Quadakkers WJ: ‘Enhanced oxidation of the 9%Cr steel P91 in water vapor containing environment’, Corros. Sci., 2006, 48, 3428–3454.
  • E. Essuman, G. H. Meier, J. Zurek, M. Hănsel: ‘The effect of water vapor on selective oxidation of Fe-Cr alloys’, Oxid. Met., 2008, 69, 143–162.
  • Topfer J, Aggarwal S and Dieckmann R: ‘Point-defects and cation tracer diffusion in (CrXFe1-X)(3-delta)O-4 spinels’, Solid State Ionics, 1995, 81, (3–4), 251–266.
  • Folkeson N, Jonsson T, Halvarsson M, Johansson L.-G and Svensson J.-E: ‘The influence of small amounts of KCl(s) on the high temperature corrosion of a Fe-2·25Cr-1Mo steel at 400 and 500 degrees C’, Mater. Corros., 2011, 62, (7), 606–615.
  • Jonsson T, Pujilaksono B, Heidari H, Liu F, Svensson JE, Halvarsson M and Johansson LG: ‘Oxidation of Fe–10Cr in O2 and in O2+H2O environment at 600°C: A microstructural investigation’, Corros. Sci., 2013, 75, 326–336.
  • B. Pujilaksono, T. Jonsson, H. Heidari, M. Halvarsson, J. E. Svensson, L. G. Johansson: ‘Oxidation of binary FeCr alloys (Fe-2·25Cr, Fe-10Cr, Fe-18Cr and Fe-25Cr) in O2 and in O2 + H2O environment at 600 C’, Oxid. Met., 2011, 75, 183–207.
  • Ueda M, Kawamura K and Maruyama T: ‘Void formation in magnetite scale formed on iron at 823 K – elucidation by chemical potential distribution’, in ‘High-temperature oxidation and corrosion 2005’ (ed. S. Taniguchi et al.), 37–44; 2006, Stafa-Zurich, Trans Tech Publications Ltd.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.