References
- Bowker M: in‘Automotive engineering lightweight, functional, and novel materials’(, Cantor B, et al..), 39–48; 2008; Boca Raton, FL, CRC Press.
- Twigg MV: Platinum Met. Rev., 2003, 47, (4), 157–162.
- Farrauto RJ, Heck RM: Catal. Today, 1999, 51, (3–4), 351–360.
- Hightower JW: AIChE Symp., 1976, 72, (156), 354–368.
- Andrews D: Patent no. 2009-1640102146071, 2009.
- Xu Z, Yi J, Wooldridge S, Reiche D, Curtis E, Papaioannou G: ‘SI combustion and direct injection SI engine technology’, SP SP-2241, 349–369; 2009, Warrendale, PA, Society of Automotive Engineers.
- Nakouzi SR, McBride JR, Nietering KE, Visser JH, Adamczyk, Jr AA, Narula CK: Proc. Materials Research Society Symp.: ‘Advanced catalytic materials’, Boston, MA, USA, December 1996, Materials Research Society, Vol. 454, 283–289.
- Kuhlwein J, Friedrich R: Atmos. Environ., 2000, 34, (27), 4603–4610.
- Hattendorf H, Hojda R, Naumenko D, Kolb-Telieps A: Mater. Corros., 2008, 59, (6), 449–454.
- Engkvist J, Bexell U, Grehk M, Olsson M: Mater. Corros., 2009, 60, (11), 876–881.
- Engkvist J, Canovic S, Liu F, Goetlind H, Svensson JE, Johansson LG, Olsson M, Halvarsson M: Mater. High Temp., 2009, 26, (2), 199–210.
- Chen L, Jha B: ‘Advanced catalysts’, SP-1864, 109–116; 2004, Warrendale, PA, Society of Automotive Engineers.
- Simms NJ, Norton JF, McColvin G: ‘Novel approaches to improving high temperature corrosion resistance’, European Federation of Corrosion Series No. 4736–64; 2008, Cambridge, Woodhead Publishing Limited.
- Xiao R, Dong P, Chen K: Laser Inst. Am., 2009, 102, 660–665.
- Ryabov VR: Weld. World, 2001, 45, 123–128.
- Eagar TW: Weld. J., 1995, 74, (6), 49–55.
- Santella ML: Am. Ceram. Soc. Bull., 1992, 71, (6), 947–954.
- Lundin CD: Weld. J., 1982, 61, (2), 58–63.
- Spain KD: in ‘Brazing and soldering’, Proc. Int. Brazing and Soldering Conf., San Antonio, TX, USA, April 2006, ASM International, 293–297.
- Perry ER: Weld. Met. Fabr., 1991, 59, (1), 11–17.
- Zatz TJ, Tobin A, Wittko J: J. Nucl. Mater., 1979, 85–86, (A), 427–431.
- Buchner S, Lardies SS, Degen A, Donnerstag A, Held W: ‘Emission control modeling’, SP-1605, 45–66; 2001, Warrendale, PA, Society of Automotive Engineers.
- Holy G, Bruck R, Hirth P: ‘Advanced three-way catalysts’, PT-123, 391–397; 2006, Warrendale, PA, Society of Automotive Engineers.
- Nagy DB, Loo J, Tulpa J, Schroeder P, Middleton R, Morgan C: ‘Emission measurement and testing’, SP-1503, 21–45; 2000, Warrendale, PA, Society of Automotive Engineers.
- Kishi N, Kikuchi S, Suzuki N, Hayashi T: ‘Advanced three-way catalysts’, PT-123, 417–425; 2006, Warrendale, PA, Society of Automotive Engineers.
- Kishi N, Kikuchi S, Suzuki N, Hayashi T: ‘Advanced converter technologies’, SP-1409, 93–100; 1999, Warrendale, PA, Society of Automotive Engineers.
- Lloyd AC: Issues Environ. Sci. Technol., 1997, 8, 141–156.
- Kell J, Tyrer JR, Higginson RL, Thomson RC: J. Microsc., 2005, 217, (2), 67–173.
- Du Toit M, Pistorius PC: Weld. J., 2003, 82, 219S–224S.
- Zacharia T, Eraslan AH, Aidun DK: Weld. J., 1988, 67, 53S–62S.
- Okabea S, Kohnoa M, Ishiia K, Yukumotoa M, Nozakia T: Mater. Sci. Eng. A, 1994, A181–A182, 1104–1108.
- Schwartz MM: ‘Brazing’, 2nd edn; 2003, Materials Park, OH, ASM International.
- Roberts PM: ‘Industrial brazing practice’; 2004, Boca Raton, FL, CRC Press.
- Jacobson DM, Humpston G: ‘Principles of brazing’, 2005, Materials Park, OH, ASM International.
- Lee D: J. Alloys Compd, 2009, 480, (2), 347–350.
- Zhao K, Ma YH, Lou LH, Hu ZQ: Mater. Sci. Eng. A, 2008, A480, 205–208.
- ArvinMeritor-Rosi Laboratories: personal communication.
- El Kadiri H, Wang L, Horstemeyer MF, Yassar RS, Berry JT, Felicelli S, Wang PT: Mater. Sci. Eng. A, 2008, A494, (1–2), 10–20.
- El Kadiri H, Molins R, Bienvenu Y, Horstemeyer MF: Oxid. Met., 2005, 64, (1/2), 99–117.
- El Kadiri H: ‘Mechanisms of High Temperature Oxidation in Alumina-Forming Alloys’, PhD thesis, Ecole des Mines de Paris at the Materials Center, Paris, France, 2004.
- El Kadiri H, Molins R, Bienvenu Y, Horstemeyer MF: Oxid. Met., 2005, 64, (1), 63–97.
- Tadmor R: J. Colloid Interface Sci., 2009, 332, (2), 451–454.
- Toguri JM, Ip SW: Proc. Alex McLean Symp., Toronto, Ont., Canada, July 1998, Iron and Steel Society, Warrendale, PA, 77–86.
- Wei PS, Chung FK: Metall. Mater. Trans. B, 2000, 31B, (6), 1387–1403.
- Lampman S: ‘Weld integrity and performance’; 1997, Materials Park, OH, ASM International.
- Semak V, Matsunawa A: J. Phys. D, 1997, 30D, (18), 2541–2552.
- El Kadiri H, Horstemeyer MF, Bammann DJ: J. Mech. Phys. Solids, 2008, 56, (12), 3392–3415.
- El Kadiri H, Molins R, Bienvenu Y: Mater. Sci. Forum, 2004, 461–464, 1107–1116.
- Jedlinski J: Solid State Ionics, 1997, 101–103, (Pt 2), 1033–1040.
- El Kadiri H, Bienvenu Y, Solanki K, Horstemeyer MF, Wang PT: ‘Creep and tensile behaviors of Fe–Cr–Al foils and laser microwelds at high temperature’, Mater. Sci. Eng. A, 2006, A421, (1), 168–181.
- Germidis A: ‘Comportement thermomécanique de structures alvéolaires pour pots catalytiques’, PhD thesis, Centre des Matériaux, Ecole Nationale Supérieure des Mines de Paris, ENSMP, Paris, France, 1996.