References
- Stoltenhoff T, Kreye H, Richter HJ and Assadi H: ‘Optimization of the cold spray process’, in ‘Thermal spray 2001: new surfaces for a millennium’, (ed. Berndt C C, Khor K A and Lugscheider E F), 409–416; 2001, Materials Park, OH, ASM International.
- Papyrin A, Kosarev V, Klinkov S, Alkhimov AP and Fomin V: ‘Cold spray technology’, (ed. Papyrin A); 2007, Amsterdam, Elsevier.
- Karthikeyan J: ‘Cold spray technology: international status and USA efforts’, 1–14; 2004, Barberton, OH, ASB Industries Inc.
- Lima RS, Karthikeyan J, Kay CM, Lindemann J and Berndt CC: Thin Solid Films, 2002, 416, 129.
- Zhao ZB, Gillispie BA and Smith JR: Surf. Coat. Technol., 2006, 200, 4746–4754.
- Villafuerte J: Met. Finish., 2010, 37–39.
- Dykhuizen RC and Smith MF: J. Therm. Spray Technol., 1998, 7, (2), 205–212.
- Shukla V, Elliott G and Kear B: Proc. 37th AIAA Aerospace Sciences Meet. and Exhibit, Reno, NV, USA, January 1999, AIAA, p1.
- McCune RC, Papyrin AN, Hall JN., Riggs WL and Zajchowski PH: in ‘Advances in thermal spray science and technology’, (ed. Berndt C C and Sampath S); 1995, Materials Park, OH, ASM International.
- Alkimov AP, Papyrin AN, Dosarev VP, Nesterovich NI and Shushpanov MM: US Patent 5,302,414, April 12, 1994.
- McCune RC, Donlon WT, Popoola OO and Cartwright EL: J. Therm. Spray Technol., 2000, 9, (1), 73–82.
- Richer P, Yanouzi M, Beauvais L and Jodoin B: Surf. Coat. Technol., 2010, 204, 3962–3974.
- Bala N, Singh H and Prakash S: J. Therm. Spray Technol., 2012, 21, 144–158.
- Sampath S, Jiang XY, Matejicek J, Prchlik L, Kulkarni A and Vaidya A: Mater. Sci. Eng. A, 2004, A364, 216–231.
- Zhou X and Mohanty P: Electrochim. Acta, 2012, 65, 134–140.
- Kim HJ, Lee CH and Hwang SY: Mater. Sci. Eng. A, 2005, A391, 243–248.
- Wolfe DE, Eden TJ, Potter JK and Jaroh AP: J. Therm. Spray Technol., 2006, 15, (3), 400–412.
- Kim JH, Lee CH and Hwang SY: Surf. Coat. Technol., 2005, 191, (2), 335–340.
- Gao PH, Li CJ, Yang GJ, Li YG and Li CX: Appl. Surf. Sci., 2010, 256, 2263–2268.
- Li CJ and Li WY: Surf. Coat. Technol., 2003, 167, (2–3), 273.
- Lima RS, Kucuk A, Berndt CC Karthikeyan J, Kay CM and Indemann J: J. Mater. Sci. Lett., 2002, 21, 1687–1689.
- Cinca N, Barbosa M, Dosta S and Guilemany JM: Surf. Coat. Technol., 2010, 205, (4), 1096–1102.
- Moy CKS, Cairney J, Ranzi G, Jahedi M and Ringer SP: Surf. Coat. Technol., 2010, 204, 3739–3749.
- Hussain T, McCartney DG, Shipway PH and Marrocco T: J. Therm. Spray Technol., 2011, 20, (1–2), 260–274.
- Balani K, Agarwal A, Seal S and Karthikeyan J: Scr. Mater., 2005, 53, 845–850.
- Ajdelsztajn L, Jodoin B, Kim GE and Schoenung JM: Metall. Mater. Trans. A, 2005, 36A, 657–666.
- Zhang D, Shipway PH and McCartney DG: J. Therm. Spray Technol., 2005, 14, (1), 109–116.
- Morgan R, Fox P, Pattison J, Sutcliffe C and Neill WO: Mater. Lett., 2004, 58, 1317–1320.
- Zhang MX, Huang H, Spencer K and Shi YN: Surf. Coat. Technol., 2010, 204, 2118–2122.
- Irissou E, Legoux JG, Arsenault B and Moreau C: J. Therm. Spray Technol., 2007, 16, (5–6), 661–668.
- Spencer K, Fabijanic DM and Zhang MX: Surf. Coat. Technol., 2009, 204, 336–344.
- Tao Y, Xiong T, Sun C, Jin H, Du H and Li T: Appl. Surf. Sci., 2009, 256, 261–266.
- Wang Q, Spencer K, Birbilis N and Zhang MX: Surf. Coat. Technol., 2010, 205, (1), 50–56.
- Shukla V, Elliott GS and Kear H: J. Therm. Spray Technol., 2000, 9, (3), 394–398.
- Koivuluoto H, Lagerbom J and Vuoristo P: J. Therm. Spray Technol., 2007, 16, (4), 488–497.
- Kairet T, Degrez M, Campana F and Janssen JP: J. Therm. Spray Technol., 2007, 16, (5–6), 610–618.
- Fukumoto M, Mashiko M, Yamada M and Yamaguchi E: J. Therm. Spray Technol., 2010, 19, (1–2), 89–94.
- King PC, Bae G, Zahiri SH, Jahedi M and Lee C: J. Therm. Spray Technol., 2010, 19, (3), 620–634.
- Koivuluoto H and Vuoristo P: J. Therm. Spray Technol., 2010, 19, (5), 1081–1092.
- Raj SV, Pawlik R and Loewenthal W: Mater. Sci. Eng. A, 2009, A513–A514, 59–63.
- Koivuluoto H and Vuoristo P: J. Therm. Spray Technol., 2009, 18, (4), 555–562.
- Kong LY, Shen L, Lu B, Yang R, Cui XY, Li TF and Xiong TY: J. Therm. Spray Technol., 2010, 19, (6), 1206–1210.
- Lee H, Shin H and Ko K: J. Therm. Spray Technol., 2010, 19, (1–2), 102–109.
- Li WY, Yang C and Liao H: Mater. Des., 2011, 32, (1), 388–394.
- Poza P, Múneza CJ, Garridoa MA, Vezzùb S, Rechb S and Trentinb A: Procedia Eng., 2011, 10, 3799–3804.
- Xiong Y, Bae G, Xiong X and Lee C: J. Therm. Spray Technol., 2010, 19, (3), 575–585.
- Bala N, Singh H and Prakash S: Appl. Surf. Sci., 2009, 255, (15), 6862–6869.
- Bala N, Singh H and Prakash S: Metall. Mater. Trans. A, 2011, 42A, 3399–3416.
- Bala N, Singh H and Prakash S: Mater. Des., 2009, 31, 244–253.
- Bala N, Singh H and Prakash S: J. Therm. Spray Technol., 2010, 19, 110–118.
- Bala N: ‘Investigations on the Hot Corrosion Behaviour of Cold Spray and HVOF Spray Coatings on T22 and SA 516 Steels’, PhD thesis, Punjab Technical University, Jalandhar, Punjab, India, 2010.
- Rahman A, Chawla V, Jayaganthan R, Chandra R, Tewari VK and Ambardar R: Surf. Eng., 2012, 28, (4), 249–256.
- Kaushal G, Kaur N, Singh H and Prakash S: Surf. Eng., 2012, 29, (1), 46–54.
- Mahesh RA, Jayaganthan R and Prakash S: Surf. Eng., 2011, 27, (5), 332–339.
- Kaur M, Singh H and Prakash S: Surf. Eng., 2010, 26, (6), 428–439.
- Kaushal G: ‘Erosion-corrosion Studies on High Velocity Oxy- fuel Thermal Spray Coating over some Boiler steels’, PhD thesis, Punjab Technical University, Jalandhar, Punjab, India, 2011.
- Sidhu HS, Sidhu BS and Prakash S: Surf. Coat. Technol., 2006, 200, (18–19), 5386–5394.
- Sidhu TS, Prakash S and Agrawal RD: Thin Solid Films, 2006, 515, (1–2), 95–105.
- Sidhu TS, Prakash S and Agrawal RD: Surf. Coat. Technol., 2006, 201, (3–4), 792–800.
- Singh H, Puri D and Prakash S: Surf. Coat. Technol., 2005, 192, 27–38.
- Singh H, Puri D and Prakash S: ISIJ Int., 2005, 45, (6), 886–895.
- Singh H: ‘Hot Corrosion Studies of Plasma Sprayed Coatings Over Some Ni- and Fe-Based Superalloys’, PhD thesis, Indian Institute of Technology, Roorkee, India, 2005.
- Sidhu BS: ‘Studies on the Role of Coatings in Improving Resistance to Hot Corrosion and Degradation’, PhD thesis, Indian Institute of Technology, Roorkee, India, 2003.
- Sidhu BS and Prakash S: Surf. Coat. Technol., 2006, 201, (3–4), 1643–1654.
- Kaushal G, Singh H and Prakash S: Oxid. Met., 2011, 76, 169–191.
- Kaushal G, Singh H and Prakash S: Mater. High Temp., 2011, 28, (1), 1–11.